FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
Hollow board | A1*T1*A2*T2*B*T3 | A1*T1*A2*T2*B*T3 | ||
| 500*6*450*6*48.5*6 | 16.4 | 20" x 1/4" x 18" x 1/4" x 2" x 1/4" | 36.2 | |
| 500*6*450*6*48.5*9 | 18.5 | 20" x 1/4" x 18" x 1/4" x 2" x 3/8" | 40.8 | |
| 650*13*550*13*98.5*12 | 52.5 | 51/2" x 1/2" x 173/8" x 1/2" x 4" x 1/2" | 116 | |
| 725*4.5*675*4.5*45*4.5 | 17.9 | 57/2" x 3/16" x 53/2" x 3/16" x 7/4" x 3/16" | 39.5 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
应用场景
结构型材-空心板(间苯)适用于对强度与跨距有要求的承重与支撑结构,例如平台走道、楼梯踏步、护栏、桥架支撑及化工、海工、市政等腐蚀性环境中的框架构件。其空心截面在保持截面刚度的同时便于拼接与开孔安装。具体场景是否适用,欢迎联系我们结合工况确认。
选型指导
选型时先根据跨距、荷载与支撑方式确定截面高度与壁厚,再结合安装节点的连接形式选择开孔或拼接方案;间苯树脂体系适用于对耐腐蚀要求较高的环境,可按介质与温度条件进一步沟通。页面所列规格为常用参考,实际尺寸、重量及力学参数请以联系我们获取的详细规格与报价为准。
产品优势
该型材以玻璃纤维为增强材料、树脂为基体,经浸透、加热模压固化并连续牵引成型,具有轻质高强、耐腐蚀、非磁性、电绝缘及易加工切割钻孔的特点。空心板结构在同等用材下可获得较大的截面惯性矩,适合高强、大跨距的支撑需求。欢迎联系我们获取材料体系与工艺说明。
询盘引导
如需确认截面尺寸、长度、颜色、表面处理及包装运输等要求,欢迎联系我们获取详细规格与报价,我们将根据您的项目工况推荐合适的规格与供货方案。批量采购、定制截面及技术选型支持均可一并沟通。
简体中文