Pultruded Grating T-3810
Request a Quote
Please feel freely to contact with us for new price .
Genius FRP
Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
|---|---|---|
Resin | 25% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 65% | E |
Filler | 8% | ATH,PR |
Others | 2% | --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 25mm
Open Area: 38%
Approx Weight (With three-core shoots): 11.8kg/m²

Liner load(units:mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 300 | 450 | 750 | 1500 | 3000 | 5950 | Load |
| 450 | 0.71 | 1.02 | 1.73 | 3.45 | 6.91 | --- | 8600 |
| 600 | 1.55 | 2.34 | 3.89 | 7.75 | --- | --- | 6427 |
| 900 | 4.83 | 7.21 | --- | --- | --- | --- | 4180 |
| 1200 | 10.8 | --- | --- | --- | --- | --- | 3018 |

Uniform load(units:mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 1000 | 1900 | 3900 | 7000 | 9500 | 19500 | Load |
| 450 | 0.66 | 1.3 | 2.62 | 5 | 6.53 | --- | 37624 |
| 600 | 1.96 | 3.89 | 7.77 | --- | --- | --- | 21087 |
| 900 | 9.02 | --- | --- | --- | --- | --- | 9158 |
| 1200 | 6.6 | 13 | --- | --- | --- | --- | 9920 |
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories

Application Scenarios
Pultruded Grating T-3810 is commonly used in industrial platforms, walkways, trench covers, stair treads and equipment operating surfaces that require load-bearing capacity and corrosion resistance. As pultruded profiles are used as load-bearing bars, it is suitable for environments requiring long spans, light weight, high strength and resistance to chemical media, such as chemical, water treatment, electroplating and marine engineering applications. To confirm suitability for specific media and working conditions, please contact us for detailed specifications and selection advice.
Selection Guidance
Selection requires comprehensive consideration of the resin system, grating thickness, load-bearing bar spacing, load-bearing direction and installation support conditions. Different resin types differ in flame retardancy and corrosion resistance, and the matching resin grade should be selected according to the actual environment. We can provide selection references based on your load, span and media conditions. Please contact us to discuss your specific requirements.
Product Advantages
Pultruded grating is assembled with pultruded I/T profiles as load-bearing bars and solid tubes or rods as connecting rods, combining high specific strength, light weight, corrosion resistance and ease of cutting and installation. Compared with traditional metal grating, it is insulating, non-magnetic and low in maintenance cost, making it suitable for long-term exposure to humid or corrosive environments. For more details on material composition and structural advantages, please contact us.
Inquiry Guide
To obtain detailed specifications, load-bearing parameters, resin options and customization solutions for Pultruded Grating T-3810, please contact us. Please provide the usage environment, size requirements and load-bearing requirements, and we will provide a quotation and technical support accordingly. All commercial terms are subject to the inquiry communication confirmed by both parties.
Operating Environment
- Pultruded FRP grating T-3810 is built from pultruded "I" or "T" shaped profile bearing bars and solid pipe or bar connecting rods, making it suitable for both indoor and outdoor industrial platforms, walkways and stair treads.
- The vinyl-type resin VEFR-25 used in this grating offers an oxygen index of 28 or above, supporting use in humid or mildly corrosive atmospheres where moisture and chemical exposure are present.
- For fire safety-critical locations with low toxicity requirements, the MP-5 phenolic-type resin option provides high flame retardancy, making the grating appropriate for enclosed or high-risk process areas.
- Contact us for the full parameter list to confirm resin selection and configuration for your specific temperature, humidity and chemical exposure conditions.