拉挤格栅 I-5010
欢迎询价。
Genius FRP
Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
Resin |
25% | OFR-25、IFR-25、VEFR-25 |
Fiberglass |
65% | E |
Filler |
8% | ATH、PR |
Others |
2% | --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |

Sand surface


Antiskid groove surface

Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 25mm
Open Area: 50%
Approx Weight (With three-core shoots): 15.1kg/m²

Liner load(units:mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
(mm) | 300 | 450 | 750 | 1500 | 3000 | 5950 | Load |
| 450 | 0.46 | 0.71 | 1.17 | 2.33 | 4.66 | 8.52 | 13808 |
| 600 | 1.11 | 1.65 | 2.74 | 5.83 | 11.2 | 18.8 | 10799 |
| 900 | 3.54 | 5.06 | 8.86 | 16.5 | 34.9 | 59.2 | 7194 |
| 1200 | 8.37 | 12.9 | 22.2 | 39.6 | --- | --- | 5362 |

Uniform load(units:mm)
Spacing |
kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Limit |
(mm) | 1000 | 1900 | 3900 | 7000 | 9500 | 19500 | Load |
| 450 | 0.91 | 1.76 | 3.27 | 5.54 | 9.32 | 15.6 | 60499 |
| 600 | 2.15 | 4.29 | 9.06 | 15.1 | 18 | 26.5 | 35429 |
| 900 | 7.83 | 12.9 | 23.7 | --- | --- | --- | 15638 |
| 1200 | 17.5 | --- | --- | --- | --- | --- | 8796 |
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories

应用场景
拉挤格栅 I-5010 适用于对耐腐蚀、轻质高强有要求的工业平台、走道、楼梯踏步及地沟盖板等场合。其结构型式也常见于污水处理、化工、海洋工程等存在潮湿或化学介质的环境。如需了解在特定工况下的适用性,欢迎联系我们获取详细规格与报价。
选型指导
选型时需综合考虑承载要求、跨距、使用环境及安装方式等因素。本产品采用拉挤“I”型材作为承重条,并以实心管或棒作为连接杆,可根据实际需求选择不同树脂体系(如邻苯、间苯、乙烯基等)以满足耐腐蚀或阻燃要求。欢迎联系我们获取详细规格与报价,我们将协助您完成选型。
产品优势
拉挤格栅 I-5010 具有轻质高强、耐腐蚀、防滑及绝缘等特性,且便于切割和安装。其结构设计在保持承载能力的同时,有效减轻了整体重量,适合对自重敏感或需频繁拆卸的场合。欢迎联系我们获取详细规格与报价,了解更多产品优势。
询盘引导
如需获取拉挤格栅 I-5010 的详细技术参数、样品或报价,请通过网站联系方式与我们联系。我们可根据您的具体应用需求提供定制化解决方案。欢迎联系我们获取详细规格与报价。
简体中文
English