拉挤格栅 HL-5020
欢迎询价。
Genius FRP
Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
Resin | 25% | OFR-25、IFR-25、VEFR-25 |
Fiberglass | 65% | E |
Filler | 8% | ATH、PR |
Others | 2% | --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 50mm
Open Area: 50%
Approx Weight (With three-core shoots): 52.24kg/m²

Liner load(units:mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m |
(mm) | 150 | 300 | 450 | 750 | 1500 | 3000 | 4500 | 6000 | 7500 |
| 600 | 0.04 | 0.08 | 0.1 | 0.18 | 0.37 | 0.71 | 1.08 | 1.42 | 1.79 |
| 750 | 0.06 | 0.12 | 0.2 | 0.33 | 0.65 | 1.3 | 1.95 | 2.62 | 3.27 |
| 900 | 0.1 | 0.22 | 0.33 | 0.55 | 1.1 | 2.19 | 3.27 | 4.37 | 5.47 |
| 1200 | 0.26 | 0.51 | 0.77 | 1.28 | 2.56 | 5.12 | 7.68 | 10.2 | 12.8 |

Uniform load(units:mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² |
(mm) | 450 | 950 | 1450 | 2450 | 4850 | 9800 | 14500 | 19500 | 24400 |
| 600 | 0.04 | 0.08 | 0.14 | 0.22 | 0.45 | 0.89 | 1.34 | 1.79 | 2.21 |
| 750 | 0.1 | 0.2 | 0.3 | 0.51 | 1.02 | 2.03 | 3.07 | 4.08 | 5.1 |
| 900 | 0.2 | 0.41 | 0.61 | 1.02 | 2.05 | 4.1 | 6.14 | 8.19 | 10.2 |
| 1200 | 0.65 | 1.28 | 1.93 | 3.21 | 6.4 | 12.8 | --- | --- | --- |
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories

应用场景
拉挤格栅 HL-5020 适用于对承重、耐腐蚀与防滑有要求的工业平台、走道、沟盖板及设备操作面。常见场合包括化工、水处理、电镀、海洋工程等潮湿或腐蚀性环境,也可用于需要绝缘或轻量化的结构部位。具体场景适配请联系我们确认。
选型指导
选型时可从承载跨度、使用环境的腐蚀介质、是否需要阻燃以及安装方式几个方面考虑,再匹配相应的树脂类型与格栅厚度。不同树脂体系在耐腐蚀和阻燃表现上各有侧重,欢迎联系我们获取详细规格与选型建议。我们可根据工况推荐合适的配置。
产品优势
拉挤格栅以拉挤“I”“T”型材作承重条、实心管或棒作连接杆组装而成,具有轻质高强、耐腐蚀、不易锈蚀的特点。相比传统金属格栅,它免于电化学腐蚀,维护成本更低,且便于切割与现场安装。整体结构稳定,适合长期暴露在恶劣环境中使用。
询盘引导
如需了解拉挤格栅 HL-5020 的具体规格、树脂选项与商务条款,欢迎联系我们获取详细规格与报价。请提供使用环境、承载要求与尺寸需求,我们将尽快为您匹配合适方案并回复。