LM Wire Rope GB 7x19
Please feel freely to contact with us for new price .
Product Details
This compacted rope construction is available in both galvanised and ungalvanised finish with either ordinary or langs lay.The construction family includes 17X7,18X7 and 19X7.For further flexibility and other performance characteristics we also supply 32X7, 35X7 and 37X7.
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006

Applications
Offshore crane rope
Deck crane rope
Pillar crane rope
Whip hoist rope
Main hoist rope
Crane rope
Breaking Loads
|
| Min Breaking Loads | Min Breaking Loads |
Diameter | Weight | (1770Mpa) | (1770Mpa) |
| mm | kg/m | KN | Kg |
| 3 | 0.03 | 5.77 | 588 |
| 4 | 0.06 | 10.3 | 1045 |
| 5 | 0.1 | 16 | 1633 |
| 6 | 0.14 | 23.1 | 2352 |
| 7 | 0.19 | 31.4 | 3202 |
| 8 | 0.24 | 41 | 4182 |
| 9 | 0.31 | 51.9 | 5293 |
| 10 | 0.38 | 64.1 | 6535 |
| 11 | 0.46 | 77.5 | 7908 |
| 12 | 0.55 | 92.3 | 9411 |
| 13 | 0.64 | 108 | 11045 |
| 14 | 0.75 | 126 | 12809 |
| 16 | 0.98 | 164 | 16731 |
| 18 | 1.23 | 208 | 21175 |
| 20 | 1.52 | 256 | 26142 |
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
选型指导
选型时请结合额定工作载荷、使用环境(如潮湿、腐蚀)及所需柔韧性,参考表中直径、重量与最小断裂荷载数据。如需协助,欢迎联系我们提供详细规格与报价。
产品优势
LM钢丝绳提供光面或镀锌表面处理,符合GB/T 20118-2006标准,规格齐全,从0.5mm到64mm,包括多种股数和芯型,适用于海上起重机、甲板起重等严苛场合。具体性能参数可联系我们获取。
询盘引导
如需了解价格、交货期或其他商业条款,欢迎联系我们获取详细规格与报价。我们的团队将根据您的需求提供专业支持。
简体中文
English