LM Rotation Resistant Wire Rope GB19X7 (6/1)
Please feel freely to contact with us for new price .
产品详情
包含17X7, 18X7 和 19X7这三种常用规格。为了进一步提高灵活性和其他性能,我们还可提供32X7, 35X7 和 37X7这些规格。
表面处理:光面或镀锌
标准:国标GB/T 20118-2006

工程应用
海上起重机钢丝绳
甲板起重钢丝绳
立柱吊车钢丝绳
起重吊索
主提升钢丝绳
吊索
断裂荷载
|
|
最小断裂荷载 |
最小断裂荷载 |
最小断裂荷载 | 最小断裂荷载 |
直径 | 重量 |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 5 | 0.1 | 14.5 | 1480 | 16.1 | 1639 |
| 6 | 0.14 | 20.9 | 2131 | 23.1 | 2360 |
| 8 | 0.26 | 37.2 | 3789 | 41.1 | 4196 |
| 10 | 0.4 | 58.1 | 5921 | 64.3 | 6557 |
| 12 | 0.58 | 83.6 | 8527 | 92.6 | 9442 |
| 13 | 0.68 | 98.1 | 10007 | 109 | 11081 |
| 14 | 0.79 | 114 | 11606 | 126 | 12852 |
| 16 | 1.03 | 149 | 15159 | 165 | 16786 |
| 18 | 1.3 | 188 | 19186 | 208 | 21245 |
| 20 | 1.6 | 232 | 23686 | 257 | 26229 |
| 22 | 1.94 | 281 | 28661 | 311 | 31737 |
| 24 | 2.31 | 334 | 34109 | 370 | 37770 |
| 26 | 2.71 | 392 | 40030 | 435 | 44327 |
通用工程钢丝绳
绿盟(LM)专门供应多股光面或镀锌钢丝绳。我们的产品直径从0.5mm到64mm不等,包括带纤维芯和钢芯的1X19、7X7、6X19、7X19、6X36、8X19、8X36、19X7和35X7各种规格。除这些常规钢丝绳外,我们还可以提供优质的特种钢丝绳。
大多数钢丝绳在苛刻的条件下工作,必须具备抗挤压、弯曲疲劳和磨损的特性。我们所有的钢丝绳都力争达到较高的性能水平,以延长使用寿命,从而提高终端用户的生产力。因此我们确保所有材料都按照钢丝绳行业的标准生产。每根钢丝绳都可以提供例如顶针眼、旋压端和楔形插座以及许多其他装配组件。另外我们还提供定制服务,我们的工程师团队可按照您的要求制造所需规格的钢丝绳。所有材料都经过认证,具有可追溯性,且符合ISO9001标准。
Selection Guide
Common specifications of LM rotation-resistant wire rope are 17×7, 18×7 and 19×7; for greater flexibility, constructions such as 32×7, 35×7 and 37×7 can be considered. When selecting, please match according to the actual working conditions in terms of diameter, breaking force requirements and surface finish (bright or galvanized). You are welcome to contact us for detailed specifications and quotations, and we will assist you in confirming a suitable model.
Product Advantages
This series of wire rope conforms to the GB/T 20118-2006 standard, and its rotation-resistant performance helps reduce kinking and spinning during lifting. The product is suitable for offshore cranes, deck cranes, pillar cranes and main hoisting applications, and is available with bright or galvanized surface finish options. To learn about the performance differences between various specifications, you are welcome to consult us further.
Inquiry Guidance
To obtain the latest data for specific diameters, breaking loads, weights and other parameters, or to confirm availability of specifications such as 32×7, 35×7 and 37×7, please contact us directly. We can recommend a suitable construction based on your working conditions and provide detailed specifications and quotations. You are welcome to send an inquiry, and we will reply as soon as possible.