拉挤格栅 I-50125
欢迎询价。
Genius FRP
Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
Resin | 25% | OFR-25、IFR-25、VEFR-25 |
Fiberglass | 65% | E |
Filler | 8% | ATH、PR |
Others | 2% | --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 32mm
Open Area: 50%
Approx Weight (With three-core shoots): 17.4kg/m²
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories

应用场景
拉挤格栅 I-50125 适用于对承载与耐腐蚀同时有要求的平台、走道、沟盖及设备操作面,常见于化工、污水处理、海洋工程与电力等湿热或腐蚀性环境。具体场景的适配性需结合跨距、荷载与介质条件确认。
选型指导
选型时请重点关注承载方向、支撑跨距、使用荷载与腐蚀介质类型,据此确定树脂体系、承载条规格与连接杆间距。欢迎联系我们提供工况参数,由我们协助推荐合适的格栅配置与树脂类型。
产品优势
采用拉挤 I 型承载条与实心管/杆连接杆组装而成,结构方向性强,在承载方向具有较高的强度重量比。FRP 材质本身耐腐蚀、不导电、免磁,便于现场切割与安装,适合替代传统金属格栅。
询盘引导
如需了解 I-50125 的详细规格、树脂选项与供货信息,欢迎联系我们,我们将根据您的项目需求提供报价与技术支持。

简体中文