Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25、IFR-25、VEFR-25

Fiberglass

33%

E

Filler

31%

ATH、PR

Others

1%

---

Introduction of raw materials

Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Feature One

Software - Sample 2 for three columns

Feature Two

Software - Sample 3 for three columns

Feature Three

83 83 H40

83*83*40(mm)

Panel size available:

1007*4007,1007*3007 Bidirectional force.

Bearing bar thickness (Top/Bottom):7.0/5.0

Bearing bar center:83

Open Aera:84%

Approx Weight:9.5kgs/m²

83 83 H40

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

Software - Sample 1 for three columns


Software - Sample 2 for three columns


Software - Sample 3 for three columns



应用场景

玻璃钢模塑格栅83*83H40的网格尺寸与40mm厚度组合,适用于需要承载与防滑的工业平台、走道、沟盖及地坪场景。其开口结构便于液体与碎屑通过,常见于化工、水处理、电镀及海洋工程等腐蚀性环境。

选型指导

选型时需结合实际载荷、跨距、支撑方式及使用环境确定树脂体系与格栅厚度。83*83H40的网格与厚度参数可与我们的模塑格栅系列其他规格对比,欢迎联系我们获取详细规格与选型建议。

产品优势

玻璃钢模塑格栅采用不饱和聚酯树脂与玻璃纤维模压成型,具有轻质高强、耐腐蚀、防滑及绝缘等特性。83*83H40的网格设计兼顾承载与开孔率,便于安装与维护。

询盘引导

如需了解玻璃钢模塑格栅83*83H40的树脂类型、颜色、表面处理及包装方式,欢迎联系我们获取详细规格与报价。我们可根据您的项目需求提供定制化方案。

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。

发送
 访  客  人  数