Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
Resin | 35% | OFR-25、IFR-25、VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH、PR |
Others | 1% | --- |
Introduction of raw materials
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




40*40*40(mm)
Panel size available:
1247*4047,1007*4047,1007*3007
Bidirectional force.
Bearing bar thickness (Top/Bottom):7.0/5.0
Bearing bar center:40
Open Aera:67%
Approx Weight:19.2kgs/m²

Liner load(units:mm)
Span in (mm) | Load in kn/m of widht (concentrated) | Maximum Recommended | Apparent E1*10^6 N-mm^2/m |
| 400 | 7.3 | 19 | 7.14 |

Uniform load(units:mm)
Span in (mm) | Load in kn/sqm (uniformed) | Maximum Recommended | Apparent E1*10^6 N-mm^2/m |
| 400 | 1.8 | 100 | 7.14 |
| 600 | 7.7 | 45 | 8.55 |

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.



应用场景
玻璃钢模塑格栅40*40H40适用于对防腐蚀、防滑与承载有要求的平台、走道、地沟盖板及设备操作面等场合,常见于化工、水处理、电力与海洋工程环境。具体工况的适配性建议结合介质、载荷与安装方式与我们沟通确认。
选型指导
选型时可从树脂体系、格栅厚度、网格尺寸与支撑跨距等维度综合考虑,例如腐蚀性介质环境可优先关注树脂耐蚀类型,承载要求较高的区域可关注格栅高度与支撑条件。欢迎联系我们,由技术人员根据您的实际工况提供选型建议与详细规格。
产品优势
模塑成型工艺使格栅整体成型、纤维与树脂分布均匀,具备轻质高强、耐腐蚀、防滑及易切割安装等特点,便于现场加工与后期维护。相比传统金属材料,其在潮湿与腐蚀性环境中更利于延长使用周期。