FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
Angle steel | A*B*T1*T2 | A*B*T1*T2 | ||
| EL25A | 25*25*3.2*3.2 | 0.33 | 1" x 1" x 1/8" x 1/8" | 0.73 |
| EL25B | 25*25*6.4*6.4 | 0.56 | 1" x 1" x 1/4" x 1/4" | 1.23 |
| EL30A | 30*30*4(75°) | 0.46 | 5/4" x 5/4" x 3/16" (75°) | 1.01 |
| EL30B | 30*30*5*5 | 0.57 | 5/4" x 5/4" x 3/16" x 3/16" | 1.26 |
| EL32 | 32*32*4*4 | 0.42 | 5/4" x 5/4" x 3/16" x 3/16" | 0.93 |
| EL38A | 38*38*5*5 | 0.68 | 3/2" x 3/2" x 3/16" x 3/16" | 1.5 |
| EL38B | 38*38*6.4*6.4 | 0.85 | 3/2" x 3/2" x 1/4" x 1/4" | 1.87 |
| EL45 | 45*45*4.8*4.8 | 0.75 | 7/4" x 7/4" x 3/16" x 3/16" | 1.65 |
| EL50A | 50*50*3.2*3.2 | 0.62 | 2" x 2" x 1/8" x 1/8" | 1.37 |
| EL50B | 50*50*6.4*6.4 | 1.14 | 2" x 2" x 1/4" x 1/4" | 2.51 |
| EL60 | 60*60*9*9 | 1.9 | 19/8" x 19/8" x 3/8" x 3/8" | 4.19 |
| EL76A | 76*76*4.8*4.8 | 1.38 | 3" x 3" x 3/16" x 3/16" | 3.04 |
| EL76B | 76*76*6.4*6.4 | 1.77 | 3" x 3" x 1/4" x 1/4" | 3.9 |
| EL76C | 76*76*9.5*9.5 | 2.57 | 3" x 3" x 3/8" x 3/8" | 5.67 |
| EL76D | 76*76*12.7*12.7 | 3.4 | 3" x 3" x 1/2" x 1/2" | 7.5 |
| EL101A | 101*101*6.4*6.4 | 2.5 | 4" x 4" x 1/4" x 1/4" | 5.51 |
| EL101B | 101*101*8*8 | 2.95 | 4" x 4" x 5/16" x 5/16" | 6.5 |
| EL101C | 101*101*9.5*9.5 | 3.48 | 4" x 4" x 3/8" x 3/8" | 7.67 |
| EL101D | 101*101*12.7*12.7 | 4.57 | 4" x 4" x 1/2" x 1/2" | 10.1 |
| EL152A | 152*152*6.4*6.4 | 3.62 | 6" x 6" x 1/4" x 1/4" | 7.98 |
| EL152B | 152*152*9.5*9.5 | 5.42 | 6" x 6" x 3/8" x 3/8" | 12 |
| EL152C | 152*152*12.7*12.7 | 7.01 | 6" x 6" x 1/2" x 1/2" | 15.5 |
| L40 | 40*22*4.0*4.0 | 0.45 | 25/16" x 7/8" x 3/16" x 3/16" | 0.99 |
| L76 | 76*15*6*6 | 0.98 | 3" x 9/16" x 1/4" x 1/4" | 2.16 |
| L100 | 100*50*6.4*6.4 | 1.8 | 4" x 2" x 1/4" x 1/4" | 3.97 |
| L145 | 145*76*10*10 | 3.85 | 23/4" x 3" x 3/8" x 3/8" | 8.49 |
| L170 | 170*76*9.5*9.5 | 4.4 | 27/4" x 3" x 3/8" x 3/8" | 9.7 |
| L180 | 180*80*8.0*8.0 | 3.89 | 7" x 25/8" x 5/16" x 5/16" | 8.58 |
| L254 | 254*40*6.4*6.4 | 3.61 | 10" x 25/16" x 1/4" x 1/4" | 7.96 |
| L70(Special) | 70*70*24*6.0 | 3.75 | 11/4" x 11/4" x 15/16" x 1/4" | 8.27 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 |
10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density |
D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
应用场景
结构型材-角钢(间苯)适用于化工、海洋、污水处理等腐蚀性环境,以及需要高强度、大跨度的结构支撑场合。间苯树脂赋予其优异的耐腐蚀和耐候性能,在户外及潮湿条件下长期使用仍能保持稳定。欢迎联系我们,了解该产品在您具体项目中的适用性。
选型指导
选型时请根据设计荷载、跨度和连接方式确定角钢的规格尺寸。不同边宽和厚度对应不同的承载能力,间苯树脂类型可满足更高的耐腐蚀要求。如需精确选型建议,欢迎联系我们获取详细规格与技术支持。
产品优势
与传统金属材料相比,FRP角钢具有轻质高强、耐腐蚀、绝缘无磁等特性,且易于切割和安装。间苯树脂体系进一步提升了产品的耐化学性和耐久性,适合严苛工业环境。欢迎联系我们获取更多产品优势信息。