结构型材-槽钢(间苯)
欢迎询价。
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
Channel steel | A*B*T1*T2 | A*B*T1*T2 | ||
| C25 | 25*14*3*3 | 0.28 | 1" x 1/2" x 1/8" x 1/8" | 0.62 |
| C26 | 26*18*3.2*3.2 | 0.3 | 1" x 11/16" x 1/8" x 1/8" | 0.66 |
| C31 | 31*23*4*4 | 0.65 | 5/4" x 15/16" x 3/16" x 3/16" | 1.43 |
| C32 | 32*13*3*3 | 0.25 | 5/4" x 1/2" x 1/8" x 1/8" | 0.55 |
| C33 | 33*29*4*4 | 0.65 | 5/4" x 19/16" x 3/16" x 3/16" | 1.43 |
| C36 | 36*30*4*4 | 0.68 | 3/2" x 5/4" x 3/16" x 3/16" | 1.5 |
| C40 | 40*24*3.2*3.2 | 0.5 | 25/16" x 15/16" x 1/8" x 1/8" | 1.1 |
| C45 | 45*28*6.4*6.4 | 1.07 | 7/4" x 9/8" x 1/4" x 1/4" | 2.36 |
| C50 | 50*14*3.2*3.2 | 0.44 | 2" x 9/16" x 1/8" x 1/8" | 0.97 |
| C52 | 52*50*6*6 | 1.63 | 33/16" x 2" x 1/4" x 1/4" | 3.59 |
| C70 | 70*30*4.5*4.5 | 0.95 | 11/4" x 5/4" x 3/16" x 3/16" | 2.09 |
| C75 | 75*35*5*5 | 1.37 | 3" x 11/8" x 3/16" x 3/16" | 3.02 |
| C76A | 76*22*6.4*6.4 | 1.31 | 3" x 7/8" x 1/4" x 1/4" | 2.89 |
| C76B | 76*38*6.4*6.4 | 1.7 | 3" x 3/2" x 1/4" x 1/4" | 3.75 |
| C80 | 80*40*10*10 | 2.7 | 25/8" x 25/16" x 3/8" x 3/8" | 5.95 |
| C90A | 90*35*5*5 | 1.49 | 7/2" x 11/8" x 3/16" x 3/16" | 3.28 |
| C90B | 90*35*8*8 | 2.1 | 7/2" x 11/8" x 5/16" x 5/16" | 4.63 |
| C102A | 102*27*3.2*3.2 | 0.91 | 4" x 1" x 1/8" x 1/8" | 2.01 |
| C102B | 102*29*4.8*4.8 | 1.45 | 4" x 9/8" x 3/16" x 3/16" | 3.2 |
| C102C | 102*30*4*4 | 1.2 | 4" x 19/16" x 3/16" x 3/16" | 2.65 |
| C102E | 102*44*4.8*4.8 | 1.65 | 4" x 7/4" x 3/16" x 3/16" | 3.64 |
| C102F | 102*44*6.4*6.4 | 2.1 | 4" x 7/4" x 1/4" x 1/4" | 4.63 |
| C117 | 117*85*5*5 | 2.7 | 37/8" x 27/8" x 3/16" x 3/16" | 5.95 |
| C120A | 120*25*5*5 | 1.52 | 19/4" x 1" x 3/16" x 3/16" | 3.35 |
| C120B | 120*30*5*5 | 1.62 | 19/4" x 19/16" x 3/16" x 3/16" | 3.57 |
| C120C | 120*40*5*5 | 1.81 | 19/4" x 25/16" x 3/16" x 3/16" | 3.99 |
| C145 | 145*25*5*5 | 1.8 | 23/4" x 1" x 3/16" x 3/16" | 3.97 |
| C150A | 150*100*6.4*6.4 | 4.1 | 6" x 4" x 1/4" x 1/4" | 9.04 |
| C150B | 150*80*10*10 | 5.5 | 6" x 25/8" x 3/8" x 3/8"
| 12.13 |
| C152A | 152*42*4.8*4.8 | 2.03 | 6" x 13/8" x 3/16" x 3/16" | 4.48 |
| C152B | 152*42*6.4*6.4 | 2.72 | 6" x 13/8" x 1/4" x 1/4" | 6 |
| C152C | 152*42*8*8 | 3.5 | 6" x 13/8" x 5/16" x 5/16"
| 7.72 |
| C152D | 152*42*9.5*9.5 | 3.95 | 6" x 13/8" x 3/8" x 3/8" | 8.71 |
| C152E | 152*51*9.5*9.5 | 4.35 | 6" x 2" x 3/8" x 3/8" | 9.59 |
| C160 | 160*48*8*8 | 3.7 | 25/4" x 15/8" x 5/16" x 5/16" | 8.16 |
| C203A | 203*56*6.4*6.4 | 3.68 | 8" x 9/4" x 1/4" x 1/4" | 8.11 |
| C203B | 203*56*9.5*9.5 | 5.34 | 8" x 9/4" x 3/8" x 3/8"
| 11.77 |
| C203C | 203*102*12.7*12.7 | 9.2 | 8" x 4" x 1/2" x 1/2" | 20.28 |
| C210A | 210*55*5*5 | 2.95 | 33/4" x 9/4" x 3/16" x 3/16" | 6.5 |
| C210B | 210*80*5*5 | 3.42 | 33/4" x 25/8" x 3/16" x 3/16" | 7.54 |
| C210C | 210*85*5*5 | 3.52 | 33/4" x 27/8" x 3/16" x 3/16" | 7.76 |
| C240A | 240*72*8*8 | 5.7 | 19/2" x 11/4" x 5/16" x 5/16" | 12.57 |
| C240B | 240*115*5*5 | 4.4 | 19/2" x 9/2" x 3/16" x 3/16"
| 9.7 |
| C254 | 254*70*12.7*12.7 | 8.9 | 10" x 11/4" x 1/2" x 1/2"
| 19.62 |
| C292 | 292*70*12.7*12.7 | 9.8 | 23/2" x 11/4" x 1/2" x 1/2" | 21.61 |
| C300 | 300*55*5*5 | 3.85 | 12" x 9/4" x 3/16" x 3/16" | 8.49 |
| C310A | 310*115*5*5 | 5.1 | 49/4" x 9/2" x 3/16" x 3/16" | 11.24 |
| C381 | 381*90*10*10 | 10.5 | 15" x 7/2" x 3/8" x 3/8" | 23.15 |
| C436 | 436*90*10*10 | 11.7 | 69/4" x 7/2" x 3/8" x 3/8" | 25.79 |
| C491 | 491*90*12*12 | 14.3 | 77/4" x 7/2" x 1/2" x 1/2"
| 31.53 |
| C610 | 610*76*6.4*6.4 | 9.2 | 24" x 3" x 1/4" x 1/4" | 20.28 |
| C902 | 902*100*10*10 | 20.6 | 71/2" x 4" x 3/8" x 3/8" | 45.42 |
| C970 | 970*40*10*10 | 19.9 | 153/4" x 25/16" x 3/8" x 3/8" | 43.87 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
应用场景
结构型材-槽钢(间苯)常用于对强度与耐腐蚀性有要求的承重与支撑部位,如平台骨架、走道支撑、栏杆立柱、设备支架及化工、水处理等腐蚀环境中的结构件。间苯树脂体系使其适用于一般腐蚀性介质接触的场合,欢迎联系我们说明您的使用环境以确认适用性。
选型指导
选型时请关注截面尺寸(A*B*T1*T2)、单位重量与所需承载跨度,并根据安装方式确认连接与开孔要求。表中列出多种规格可供对照,若不确定选哪一款,欢迎联系我们提供工况条件,由我们协助推荐合适规格。
产品优势
槽钢采用玻璃纤维增强材料与间苯树脂,经拉挤成型,具备轻质高强、耐腐蚀、绝缘无磁等复合材料共有的特点,便于现场切割与安装。相比传统金属槽钢,在腐蚀环境中更能减少维护需求,适合对耐久性有要求的项目。
询盘引导
如需详细规格、尺寸公差、供货形式与报价,欢迎联系我们。请告知所需规格、数量与使用环境,我们将尽快为您提供支持。

简体中文
English