  FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

Flat tube

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Flat tube

A*B*T1*T2


A*B*T1*T2


FT4444*25*3.2*3.20.8

7/4" x 1" x 1/8" x 1/8"

1.76
FT50A51*25*3*30.79

2" x 1" x 1/8" x 1/8"

1.74
FT50B51*25*6.4*6.41.54

2" x 1" x 1/4" x 1/4"

3.4
FT7676*35*3*61.55

3" x 11/8" x 1/8" x 1/4"

3.42
FT8080*60*5*52.5

25/8" x 19/8" x 3/16" x 3/16"

5.51
FT91A91*38*4*41.78

7/2" x 3/2" x 3/16" x 3/16"

3.92
FT112A112*91*6.4*6.44.46

9/2" x 7/2" x 1/4" x 1/4"

9.83
FT120120*45*3*32

19/4" x 7/4" x 1/8" x 1/8"

4.41
FT175175*50*9*97

55/8" x 2" x 3/8" x 3/8"

15.4

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

Application:

  Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.  

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


应用场景

结构型材-扁管(乙烯基)广泛应用于化工、海洋、电力等对耐腐蚀要求较高的领域,常见于平台栏杆、支撑结构、走道格栅框架等。扁管截面便于连接和安装,适合需要轻质高强、绝缘无磁的场合。

选型指导

选型时请根据实际载荷、跨距及使用环境,结合扁管的截面尺寸和壁厚进行选择。我们提供多种规格,可满足不同结构需求。如需精确选型建议,欢迎联系我们获取详细规格与技术支持。

产品优势

采用乙烯基树脂,具有优异的耐腐蚀性和耐候性;玻璃纤维增强赋予其高强度、轻质的特点。拉挤工艺确保产品尺寸稳定、表面光洁,且具备绝缘、无磁、免维护等优势。

询盘引导

如需了解结构型材-扁管(乙烯基)的详细规格、价格及供货信息,欢迎联系我们获取详细规格与报价。我们的技术团队将为您提供专业选型建议和定制方案。

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。

发送
 访  客  人  数