Pultruded Grating T-5020

Pultruded Grating T-5020

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Genius FRP    

  Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.  

Name

Contect

Type

Resin

25%

OFR-25,IFR-25,VEFR-25

Fiberglass

65%

E

Filler

8%

ATH,PR

Others

2%

---

Introduction of raw materials 
Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

 The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Sand surface
Software - Sample 2 for three columns

Smooth surface
Software - Sample 3 for three columns

Antiskid groove surface

T5020

Standard Panel Size:
1220mm,915mm-wide  3050mm,6100mm-length
Bearing Bar: 50mm
Open Area: 50%

Approx Weight (With three-core shoots): 15.66kg/m²
Liner load

Liner load(units:mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Limit

(mm)

300450750150030005950

Load

6000.250.51
0.761.272.294.57---
9000.761.271.783.36.112.2---
12001.522.293.566.613.527.2---
15002.543.816.3512.524.649.5---
Uniform load

Uniform load(units:mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Limit

(mm)

1000190039007000950019500

Load

6000.510.761.272.293.056.35---
9001.022.033.816.869.4------
12003.36.3512.5------------
15006.8613.5---------------

The characteristics:

  • Fire Retardant

  • High Flame Resistance

  • Low Smoke and Toxic Fume Emissions

  • High Strength-to-Weight Ratio

  • Corrosion Resistant

  • Low Maintenance

  • Slip Resistant

  • Electrically & Thermally Non-Conductive

  • Easily Fabricated

  • Impact Resistant 

  • UV resistance

  • Maintenance free

Installation and accessories  

Installation and accessories

Application Scenarios

Pultruded Grating T-5020 is assembled with pultruded "I" and "T" profiles as load-bearing bars and solid tubes or rods as connecting rods. It is suitable for industrial platforms, walkways, trench covers, and equipment operating surfaces that require load-bearing capacity, corrosion resistance, and ventilation/drainage. Different resin systems correspond to different service environments. For specific application suitability, please contact us for confirmation.

Selection Guide

During selection, consider resin type, load-bearing requirements, and the corrosiveness and fire safety requirements of the service environment. For example, for applications with high fire safety requirements, phenolic resin systems may be considered; for general corrosion-resistant applications, vinyl ester systems may be considered. We welcome you to contact us with your operating conditions, and we will assist you in determining the appropriate specifications and configuration.

Product Advantages

Pultruded grating combines the characteristics of FRP materials, including light weight, high strength, corrosion resistance, non-conductivity, and ease of installation. Its assembled structure facilitates cutting and on-site adjustments. Compared with traditional metal gratings, it is more conducive to long-term use and maintenance in humid or corrosive environments. For specific performance data, please contact us for detailed technical information.

Inquiry Guide

For detailed specifications, resin options, load-bearing parameters, and commercial terms of Pultruded Grating T-5020, please contact us to obtain detailed specifications and a quotation. Please provide your service environment, dimensional requirements, and quantity, and we will provide selection recommendations and solutions as soon as possible.

立即联系我们,我们将有专业人员为您服务。

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send