Pultruded Grating T-3810

Pultruded Grating T-3810

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Genius FRP  

  Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.  

Name

Contect

Type

Resin

25%

OFR-25,IFR-25,VEFR-25

Fiberglass

65%

E

Filler

8%

ATH,PR

Others

2%

---

Introduction of raw materials 
Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Sand surface
Software - Sample 2 for three columns

Smooth surface
Software - Sample 3 for three columns

Antiskid groove surface

T3810

Standard Panel Size:
1220mm,915mm-wide  3050mm,6100mm-length
Bearing Bar: 25mm
Open Area: 38%

Approx Weight (With three-core shoots): 11.8kg/m²
Liner load

Liner load(units:mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Limit

(mm)

300450750150030005950

Load

4500.711.021.733.456.91---8600
6001.552.343.897.75------6427
9004.837.21------------4180
120010.8---------------3018
Uniform load

Uniform load(units:mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Limit

(mm)

1000190039007000950019500

Load

4500.661.32.6256.53---37624
6001.963.897.77---------21087
9009.02---------------9158
12006.613------------9920

The characteristics:

  • Fire Retardant

  • High Flame Resistance

  • Low Smoke and Toxic Fume Emissions

  • High Strength-to-Weight Ratio

  • Corrosion Resistant

  • Low Maintenance

  • Slip Resistant

  • Electrically & Thermally Non-Conductive

  • Easily Fabricated

  • Impact Resistant 

  • UV resistance

  • Maintenance free

Installation and accessories  

Installation and accessories

Application Scenarios

Pultruded Grating T-3810 is commonly used in industrial platforms, walkways, trench covers, stair treads and equipment operating surfaces that require load-bearing capacity and corrosion resistance. As pultruded profiles are used as load-bearing bars, it is suitable for environments requiring long spans, light weight, high strength and resistance to chemical media, such as chemical, water treatment, electroplating and marine engineering applications. To confirm suitability for specific media and working conditions, please contact us for detailed specifications and selection advice.

Selection Guidance

Selection requires comprehensive consideration of the resin system, grating thickness, load-bearing bar spacing, load-bearing direction and installation support conditions. Different resin types differ in flame retardancy and corrosion resistance, and the matching resin grade should be selected according to the actual environment. We can provide selection references based on your load, span and media conditions. Please contact us to discuss your specific requirements.

Product Advantages

Pultruded grating is assembled with pultruded I/T profiles as load-bearing bars and solid tubes or rods as connecting rods, combining high specific strength, light weight, corrosion resistance and ease of cutting and installation. Compared with traditional metal grating, it is insulating, non-magnetic and low in maintenance cost, making it suitable for long-term exposure to humid or corrosive environments. For more details on material composition and structural advantages, please contact us.

Inquiry Guide

To obtain detailed specifications, load-bearing parameters, resin options and customization solutions for Pultruded Grating T-3810, please contact us. Please provide the usage environment, size requirements and load-bearing requirements, and we will provide a quotation and technical support accordingly. All commercial terms are subject to the inquiry communication confirmed by both parties.

Operating Environment

  • Pultruded FRP grating T-3810 is built from pultruded "I" or "T" shaped profile bearing bars and solid pipe or bar connecting rods, making it suitable for both indoor and outdoor industrial platforms, walkways and stair treads.
  • The vinyl-type resin VEFR-25 used in this grating offers an oxygen index of 28 or above, supporting use in humid or mildly corrosive atmospheres where moisture and chemical exposure are present.
  • For fire safety-critical locations with low toxicity requirements, the MP-5 phenolic-type resin option provides high flame retardancy, making the grating appropriate for enclosed or high-risk process areas.