Pultruded Grating T-1210
Request a Quote
Please feel freely to contact with us for new price .
Genius FRP
Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
|---|---|---|
Resin | 25% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 65% | E |
Filler | 8% | ATH,PR |
Others | 2% | --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 25mm
Open Area: 12%
Approx Weight (With three-core shoots): 14.5kg/m²

Liner load(units:mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 150 | 300 | 450 | 750 | 1500 | 3000 | Load |
| 450 | 0.25 | 0.51 | 0.76 | 1.27 | 2.29 | 4.83 | 6482 |
| 600 | 0.51 | 1.02 | 1.52 | 2.29 | 4.83 | 9.65 | 4857 |
| 900 | 1.52 | 3.05 | 4.83 | 7.87 | --- | --- | 3233 |
| 1200 | 3.56 | 7.37 | 10.9 | --- | --- | --- | 2429 |

Uniform load(units:mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 450 | 950 | 1450 | 2400 | 4850 | 9500 | Load |
| 450 | <0.25 | 0.25 | 0.76 | 1.02 | 2.29 | 4.57 | 14933 |
| 600 | 0.51 | 1.27 | 1.78 | 3.05 | 6.1 | 12.2 | 11175 |
| 900 | 2.79 | 5.84 | 8.89 | --- | --- | --- | 7076 |
| 1200 | 9.14 | --- | --- | --- | --- | --- | 3562 |
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories

Application Scenarios
Pultruded Grating T-1210 is commonly used in industrial platforms, walkways, trench covers and equipment operating surfaces that require high load capacity, corrosion resistance and slip resistance, and is particularly suitable for wet, acid-base or rust-prone environments. Please confirm the specific working conditions with us based on the medium, span and load conditions.
Selection Guide
When selecting, we recommend clarifying the load bar specifications and spacing, grating thickness, resin system (such as orthophthalic, isophthalic, vinyl ester or phenolic, etc.) and surface anti-slip requirements, then determining the solution in combination with the corrosiveness and fire protection needs of the service environment. You are welcome to contact us, and our technical staff will assist you in completing the selection.
Product Advantages
Pultruded grating uses pultruded profiles as load bars, with fibers continuously distributed along the load-bearing direction, so it has high load-bearing efficiency and good stiffness, and is lightweight, corrosion-resistant and easy to cut and install. Compared with metal grating, it is less prone to rust in wet and corrosive environments and has lower maintenance costs.
Inquiry Guide
For detailed specifications, resin options, load data and quotations for Pultruded Grating T-1210, you are welcome to contact us and provide your service environment and dimension requirements. We can provide targeted product recommendations and commercial solutions according to your working conditions.
Operating Environment
- Pultruded FRP grating T-1210 is built with a fiberglass-reinforced polymer matrix and is formulated to resist corrosion from acids, alkalis, salts and many industrial solvents, making it suitable for both indoor and outdoor installations.
- The grating is designed for service in chemical processing plants, wastewater treatment facilities, cooling towers, and marine or offshore platforms where moisture and aggressive media are present.
- It performs reliably across a wide range of ambient temperatures and humidity levels typical of industrial operations, without the swelling or degradation associated with traditional materials.
- Its non-conductive nature and resistance to UV exposure allow it to be used in outdoor walkways, platforms and stair treads over extended periods. For specific temperature or chemical concentration limits, please contact us for the full parameter list.