FRP Molded Grating 40*40H25

FRP Molded Grating 40*40H25

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Genius FRP  

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type    

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

40 40 25

40*40*25(mm)

Panel size available:

1247*4047,1007*4047,1007*3007 

Bidirectional force.

Bearing bar thickness (Top/Bottom):7.0/5.0

Bearing bar center:40

Open Aera:67%

Approx Weight:12.3kgs/m²

Liner load

Liner load(units:mm)

 Span in (mm)

Load in kn/m of widht (concentrated)

Maximum Recommended

Apparent E1*10^6 N-mm^2/m

4004.7197.14
60013.2138.55
Uniform load

Uniform load(units:mm)

 Span in (mm)

Load in kn/sqm (uniformed)

Maximum Recommended

Apparent E1*10^6 N-mm^2/m

4001.21007.14
6004.9458.55
80014.8269.02
40 40 25

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in: 

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

40 40 25
40 40 25
40 40 25

Application Scenarios

FRP molded grating 40*40H25 is widely used for operating platforms, stair treads, trench covers and fencing in chemical, petroleum, power and wastewater treatment industries. Its corrosion resistance makes it suitable for humid, acid and alkali corrosive environments. Contact us to learn more detailed application cases.

Selection Guide

Selection requires comprehensive consideration of load requirements, span, corrosive environment and fire rating. Different resin types (such as orthophthalic, isophthalic, vinyl ester and phenolic) suit different working conditions; for example, phenolic type offers excellent flame retardant performance. For professional selection advice, please contact our technical team for detailed specifications and quotations.

Product Advantages

FRP molded grating offers advantages such as light weight and high strength, corrosion resistance, slip resistance, insulation and maintenance-free operation. Its mesh structure design facilitates installation and cutting, and its long service life can reduce long-term maintenance costs. Contact us for more information on product advantages.

Inquiry Guidance

To obtain detailed specifications, technical parameters or quotations for FRP molded grating 40*40H25, please contact us through the website. We can provide customized solutions according to your needs and serve you wholeheartedly.

Operating Environment

  • Built for outdoor installations such as walkways, platforms and stair treads, where the molded FRP grating is exposed to direct sunlight, rain and temperature swings without the corrosion problems of steel.
  • Suitable for indoor plant areas with high humidity, washdown or condensation, because the unsaturated polyester resin and E-glass fiber construction does not rust or conduct heat like metal.
  • Suited to chemically aggressive surroundings — including isophthalic, vinyl ester and bisphenol resin grades against acids, alkalis and solvents — making it a common choice for chemical, wastewater and coastal service environments.
  • The 40*40H25 molded grid pattern allows air, water and light to pass through, helping to limit standing water, debris accumulation and heat build-up on the panel surface in service.

立即联系我们,我们将有专业人员为您服务。

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send