FRP Molded Grating 38×38 H30 Heavy-Duty Type
Request a Quote
Please feel freely to contact with us for new price .
Resin type
Code | Resin type | Flame retardant property |
Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




38*38*30(mm)
Panel size available:
1220*3660,1220*2440,915*3050
Bidirectional force.
Bearing bar thickness (Top/Bottom):10.5/9.0
Bearing bar center:38
Open Aera:56%
Approx Weight:25kgs/㎡

Liner load(units:mm)
Deflcvtion | kg/m |
Limit | |||||
|---|---|---|---|---|---|---|---|
Span (mm) | 150 | 300 | 450 | 600 | 750 | 1500 |
Load |
| 300 | 0.36 | 0.48 | 0.61 | 0.76 | 0.89 | 1.06 | 17116 |
| 600 | 0.66 | 1.25 | 1.85 | 2.46 | 3.07 | 8.48 | 8718 |
| 900 | 1.80 | 3.68 | 5.56 | 7.42 | 9.30 | 13.8 | 5817 |
| 1200 | 4.75 | 9.68 | 14.6 | 19.6 | 21.2 | --- | 3755 |

Uniform load(units:mm)
Deflcvtion |
|
|
|
kg/m² |
|
|
|
|---|---|---|---|---|---|---|---|
Span (mm) | 240 | 480 | 980 | 1450 | 2450 | 3650 | 4880 |
| 300 | 0.09 | 0.19 | 0.38 | 0.49 | 0.78 | 1.05 | --- |
| 600 | 0.43 | 0.81 | 1.55 | 2.31 | 3.84 | 5.74 | --- |
| 900 | 1.70 | 3.45 | 6.96 | 10.47 | 17.5 | 23.3 | --- |
| 1200 | 5.97 | 12.2 | 24.5 | 32.6 | 38.7 | --- | --- |

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.



Application Scenarios
FRP molded grating 38×38 H30 heavy-duty type is suitable for industrial platforms, walkways, trench covers and equipment operating surfaces that require relatively high load-bearing capacity and corrosion resistance. Its grid structure and resin system can adapt to environments with moisture or corrosive media in chemical, water treatment, power and other industries. For specific suitability, we recommend confirming with us based on your operating conditions.
Selection Guide
When selecting, please consider load-bearing requirements, support span, type of corrosive media and installation method, and match them with the resin system and grating thickness. This product is a heavy-duty molded grating with 38×38 mm mesh and 30 mm thickness. If you need to compare selections under different load conditions, please contact us for detailed specifications and technical support.
Product Advantages
Molded grating is integrally formed from resin and fiberglass, featuring light weight, high strength, corrosion resistance, slip resistance and insulation, and is easy to cut and install. The heavy-duty structure improves load-bearing performance while maintaining open area, making it suitable for applications with requirements for strength and durability.
Inquiry Guide
If you would like to know the detailed specifications, resin system options and commercial terms of FRP molded grating 38×38 H30 heavy-duty type, please contact us for specifications and a quotation. We will provide a suitable solution based on your project requirements.