FRP Molded Grating 25*100H25 Heavy-Duty Type
Request a Quote
Please feel freely to contact with us for new price .
Genius FRP
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
|---|---|---|
Resin | 35% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH,PR |
Others | 1% | --- |
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasio |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




25*100*25(mm)
Panel size available:
1220*3660,1220*2440,915*3050 Width stress
Bearing bar thickness (Top/Bottom):9.5/8.0
Bearing bar center:25
Open Aera:52%
Approx Weight:19.5kgs/m²

Liner load(units:mm)
Deflcvtion | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
|---|---|---|---|---|---|---|---|
Span( mm) | 75 | 150 | 300 | 450 | 750 | 1500 | Load |
| 300 | <0.25 | 0.25 | 0.76 | 1.02 | 1.27 | 1.52 | 10058 |
| 450 | 0.51 | 0.76 | 1.78 | 2.54 | 3.3 | 4.32 | 7264 |
| 600 | 0.76 | 1.78 | 3.56 | 5.08 | 6.86 | --- | 5774 |
| 750 | 1.52 | 3.05 | 6.1 | 9.14 | 11.9 | --- | 4843 |
| 900 | 2.29 | 4.83 | 9.65 | --- | --- | --- | 4172 |
| 1050 | 3.56 | 7.11 | --- | --- | --- | --- | 3688 |
| 1200 | 5.08 | 10.2 | --- | --- | --- | --- | 3502 |

Uniform load(units:mm)
Deflcvtion | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Limit |
|---|---|---|---|---|---|---|---|
Span( mm) | 250 | 350 | 300 | 750 | 1000 | 1500 | Load |
| 300 | <0.25 | <0.25 | <0.25 | 0.25 | 0.51 | 0.51 | 32940 |
| 450 | 0.51 | 0.51 | 0.76 | 1.27 | 1.52 | 2.29 | 18910 |
| 600 | 1.02 | 1.27 | 2.03 | 3.3 | 4.32 | 6.35 | 15860 |
| 750 | 2.29 | 3.05 | 4.57 | 7.11 | 9.4 | --- | 12688 |
| 900 | 4.57 | 5.84 | 8.89 | --- | --- | --- | 9111 |
| 1050 | 7.87 | 10.2 | --- | --- | --- | --- | 6900 |
| 1200 | 12.7 | --- | --- | --- | --- | --- | 5734 |

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRPgrating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
Application Scenarios
FRP molded grating 25*100H25 heavy-duty type is suitable for industrial platforms, walkways, trench covers and equipment operating surfaces that require high load-bearing capacity and corrosion resistance. Its 25 mm thickness and 100 mm mesh structure maintain ventilation and light transmission while accommodating relatively heavy loads. For specific application suitability, please contact us for detailed specifications and a quotation.
Selection Guide
During selection, the actual load, span, support method and corrosive environment should be considered to confirm whether the resin type and grating thickness match. This product is the 25*100H25 heavy-duty type. If you are unsure about your working conditions, please contact us for detailed specifications and a quotation, and our technical staff will help confirm a suitable model.
Product Advantages
FRP molded grating features light weight, high strength, corrosion resistance, anti-slip performance and insulation. The molded process interweaves the mesh and load-bearing bars as one, giving good structural integrity. The heavy-duty type enhances load-bearing capacity while maintaining the corrosion resistance advantages of FRP, making it suitable for areas with higher structural strength requirements. Please contact us for detailed specifications and a quotation.
Inquiry Guidance
If you would like to know the resin type, color, surface treatment and supply information of FRP molded grating 25*100H25 heavy-duty type, please contact us for detailed specifications and a quotation. Please provide your working conditions and quantity requirements, and we will match a solution for you as soon as possible.
Operating Environment
- Designed for industrial service in both indoor and outdoor environments where the FRP molded grating may be exposed to moisture, humidity and intermittent water contact.
- Suitable for areas with chemical splash, vapours and corrosive media typically found in process, treatment and utility plants; the resin system selected for this grating must be matched to the specific chemicals present.
- Performs in outdoor installations exposed to sunlight and weather, since the fiberglass-reinforced plastic construction with UV-stabilised resin and E-glass reinforcement is intended for long-term exterior use.
- Intended for heavy-load walkways, platforms, trench covers and stair treads in industrial operating areas; actual load, support span, chemical exposure and service conditions must be confirmed with our technical team before order.