Breaking load
Diameter
| Weight
|
Minimum breaking load (1570MPa)
|
Minimum breaking load (1570MPa)
|
|---|---|---|---|
mm | kg/m | KN |
Kg |
| 6 | 0.14 | 18.5 | 1887 |
| 8 | 0.26 | 33 | 3366 |
| 9 | 0.32 | 41.7 | 4253 |
| 10 | 0.4 | 51.5 | 5253 |
| 11 | 0.5 | 62.3 | 6354 |
| 12 | 0.58 | 74.2 | 7568 |
| 13 | 0.68 | 87.1 | 8884 |
| 14 | 0.8 | 101 | 10302 |
| 16 | 1.04 | 132 | 13464 |
| 18 | 1.32 | 167 | 17034 |
| 19 | 1.44 | 186 | 18972 |
| 20 | 1.62 | 206 | 21012 |
| 22 | 2.04 | 249 | 25398 |
General engineering wire rope
Greenlogy TEC (LM) specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these standard wire ropes, we can also provide high-quality specialty wire ropes.
Most wire ropes work under demanding conditions and must be resistant to crushing, bending fatigue and wear. All our wire ropes strive to achieve a high performance level to extend service life, thereby improving end-user productivity. We therefore ensure that all materials are produced in accordance with wire rope industry standards. Each wire rope can be supplied with fittings such as thimbles, swaged terminals and wedge sockets, as well as many other assembly components. We also offer customization services; our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable and compliant with ISO9001 standards.
Selection Guide
Greenlogy TEC (LM) rotation-resistant wire rope (GB18X7 (6/1)) is suitable for applications requiring low rotation characteristics, such as marine cranes, marine and seawater environments, sewage treatment plants, wire rope slings and hoisting ropes. When selecting, please comprehensively evaluate factors such as the working load, operating environment, diameter and length, surface treatment (bright or galvanized) and wire rope construction. You are welcome to contact us with your specific application and parameter requirements, and we will help you confirm the appropriate specification.
Product Advantages
Greenlogy TEC (LM) rotation-resistant wire rope (GB18X7 (6/1)) is produced in accordance with the national standard GB/T 20118-2006, with bright or galvanized surface treatment options, and offers good rotation resistance, making it suitable for engineering applications requiring low rotation. Its structural design helps maintain stability under dynamic working conditions and reduces the risk of wear caused by rotation. For more detailed performance characteristics, please contact us.
Inquiry Guidance
To obtain detailed specifications, quotations or customization solutions for Greenlogy TEC (LM) rotation-resistant wire rope (GB18X7 (6/1)), please contact us. Please provide information such as the required diameter, length, surface treatment and quantity, and we will reply as soon as possible with professional support.