LM Filler Wire Rope GB6X19 (12/6+6F/1) FC
Product details
Product Details
The core of 6X19 filler wire rope (often referred to as 6x25) includes FC (fiber core) and IWRC (independent wire rope core).6X19 Filler wire rope Due to the fiber core, service life is usually longer than other 6X19 wire ropes.6X19 filler wire rope can bear loads of 1T-5T and is used as wire rope slings.This construction is widely used in the North Sea oil industry.
Surface treatment: bright or galvanized
Standard: GB/T 20118-2006
Engineering Applications
Drilling line
Elevator hoisting rope
Wire rope slings
Luffing wire rope
Hoisting rope
Crane wire rope
Sand line, coring line and swabbing line
Trawl fishing / ocean sweeping
Grounding rope / ground drag rope
Oil well / oilfield
Excavator rope / scraper rope
Fishing line
Tow rope
Breaking load
|
|
Minimum breaking load |
Minimum breaking load |
Minimum breaking load | Minimum Breaking Load |
|---|---|---|---|---|---|
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 14 | 0.7 | 114 | 11677 | 127 | 12930 |
| 16 | 0.92 | 150 | 15252 | 166 | 16889 |
| 18 | 1.16 | 189 | 19303 | 210 | 21375 |
| 20 | 1.44 | 234 | 23831 | 259 | 26389 |
| 22 | 1.74 | 283 | 28835 | 313 | 31931 |
| 24 | 2.07 | 336 | 34317 | 373 | 38000 |
| 26 | 2.43 | 395 | 40274 | 437 | 44598 |
| 28 | 2.82 | 458 | 46709 | 507 | 51723 |
| 30 | 3.23 | 526 | 53620 | 582 | 59376 |
| 32 | 3.68 | 598 | 61008 | 662 | 67556 |
| 34 | 4.15 | 675 | 68872 | 748 | 76265 |
| 36 | 4.65 | 757 | 77213 | 838 | 85501 |
| 38 | 5.18 | 843 | 86030 | 934 | 95265 |
| 40 | 5.74 | 935 | 95325 | 1035 | 105557 |
| 42 | 6.33 | 1030 | 105095 | 1141 | 116377 |
| 44 | 6.95 | 1131 | 115343 | 1252 | 127724 |
| 46 | 7.6 | 1236 | 126067 | 1369 | 139600 |
| 48 | 8.27 | 1346 | 137268 | 1490 | 152003 |
General Engineering Wire Rope
Greenlogy TEC LM specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5 mm to 64 mm and include 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 constructions with fiber core and steel core. In addition to these conventional wire ropes, we can also supply premium special wire ropes.
Most wire ropes work under demanding conditions and must resist crushing, bending fatigue and wear. All our wire ropes strive for a high performance level to extend service life and thereby improve end-user productivity. We therefore ensure that all materials are produced in accordance with wire rope industry standards. Every wire rope can be supplied with fittings such as thimbles, swaged terminals and wedge sockets as well as many other assembly components. We also offer customization: our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable and conform to ISO9001.
Selection Guide
When selecting, first confirm the wire rope's application, required diameter range, surface finish (bright or galvanized) and core type (FC fiber core or IWRC independent wire rope core), then match the safety factor against the breaking load data in the table above. If the working conditions involve frequent bending, corrosive environments or heavy-load lifting, welcome to contact us for detailed specifications and a quotation, and our technical staff will help confirm the suitable construction.
Product Advantages
The 6X19 filler wire rope uses a fiber core construction and offers good flexibility, typically achieving a longer service life at the same diameter, and can be supplied with bright or galvanized surface finish as required to suit a variety of lifting and towing applications. The product is manufactured in accordance with the national standard GB/T 20118-2006 and covers applications such as drilling lines, elevator ropes, rigging and oilfield ropes.
Inquiry Guide
For specific diameter, core, surface finish and packaging method, welcome to contact us for detailed specifications and a quotation. Please provide your application, required diameter range and quantity, and we will recommend a suitable model accordingly and confirm the commercial terms.
Operating Environment
- Suited to outdoor and indoor working positions where the 6X19 filler wire rope with fiber core is exposed to weather, including the drilling line, hoisting rope and luffing wire rope duties listed for this product.
- The fiber core (FC) construction and the bright or galvanized surface treatment allow this wire rope to serve in humid or moisture-bearing surroundings; galvanized versions are the usual choice where corrosion exposure is a concern.
- Because the construction is widely used in the North Sea oil industry, it is intended for offshore and other corrosive-atmosphere sites, as well as for wire rope slings and elevator hoisting rope in general plant conditions.
- For crane wire rope, sand line and similar applications, keep the rope away from sustained contact with acid, alkali or other aggressive media; specify galvanized or a protective coating and confirm suitability with us for such sites.