LM Compacted Non-rotating Wire Rope GB37X7 (6/1)
Product details
Product Details
37x7 wire rope is available in both galvanized and non-galvanized options. Based on your requirements for higher breaking load and better wear characteristics, we can apply surface treatment, lubrication, plastic coating and compaction.
Surface treatment: bright or galvanized
Standard: GB/T 20118-2006
Engineering Applications
Offshore crane wire rope
Deck crane wire rope
Pillar crane wire rope
Lifting slings
Main hoist wire rope
Slings
Breaking load
|
|
Minimum breaking load |
Minimum breaking load |
Minimum breaking load | Minimum breaking load |
|---|---|---|---|---|---|
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 14 | 0.95 | 154 | 15708 | 171 | 17442 |
| 15 | 1.09 | 177 | 18054 | 196 | 19992 |
| 16 | 1.25 | 203 | 20706 | 225 | 22950 |
| 18 | 1.58 | 257 | 26214 | 285 | 29070 |
| 19 | 1.78 | 290 | 29580 | 321 | 32742 |
| 20 | 1.95 | 318 | 32436 | 352 | 35904 |
| 21 | 2.15 | 349 | 35598 | 387 | 39474 |
| 22 | 2.37 | 385 | 39270 | 426 | 43452 |
| 23 | 2.56 | 416 | 42432 | 461 | 47022 |
| 24 | 2.81 | 457 | 46601 | 506 | 51612 |
| 25 | 3.1 | 504 | 51510 | 558 | 56916 |
| 26 | 3.3 | 537 | 54774 | 595 | 60690 |
| 28 | 3.8 | 618 | 63036 | 685 | 69870 |
| 29 | 4.1 | 667 | 68034 | 738 | 75276 |
| 30 | 4.45 | 724 | 73848 | 802 | 81804 |
| 32 | 4.96 | 806 | 82212 | 892 | 90984 |
General engineering wire rope
Greenlogy TEC (LM) specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these standard wire ropes, we can also supply high-quality special wire ropes.
Most wire ropes work under demanding conditions and must be resistant to crushing, bending fatigue and wear. All our wire ropes strive to achieve high performance levels to extend service life and thereby improve end-user productivity. We therefore ensure that all materials are produced in accordance with wire rope industry standards. Every wire rope can be supplied with fittings such as thimble eyes, swaged terminals and wedge sockets, as well as many other assembly components. We also offer customization services, and our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable and compliant with ISO9001.
Selection Guide
Please select according to your specific application, required diameter, surface treatment (bright or galvanized) and breaking load requirements. We can provide customized surface treatment, lubrication, plastic coating and compaction services. Contact us for detailed specifications and quotations.
Product Advantages
LM compacted rotation-resistant wire rope (GB37X7) offers higher breaking load and better wear resistance, making it suitable for demanding environments such as offshore cranes, deck cranes and pillar cranes. Its rotation-resistant design reduces twisting during lifting, improving operational safety and stability.
Inquiry Guidance
For more product information, technical parameters, or business cooperation, please contact us through our website or email. We look forward to providing you with professional solutions and quotations.
Operating Environment
- This compacted 37x7 wire rope is suited to outdoor and offshore service, where it is exposed to atmospheric humidity, salt-laden air and repeated wetting; the galvanized option is intended for such corrosive conditions.
- Typical operating locations include deck crane, pillar crane and main hoist installations on vessels and at ports, as well as lifting slings used in industrial yards.
- The rope operates across a wide ambient temperature range typical of marine and industrial sites; for extreme temperatures or specific corrosive media, contact us to discuss surface treatment, lubrication or plastic coating.
- Where the rope runs over sheaves and drums in dusty or abrasive outdoor environments, the compacted strand and the choice of bright or galvanized finish help it withstand the wear encountered in these conditions.