LM (Coating) Filler Compacted Wire Rope GB6X19 (12/6+6F/1) FC
Product details
Product Details
6X19 coated compacted filler wire rope (often referred to as 6x25) has a core available in FC (fiber core) and IWRC (independent wire rope core). 6X19 wire rope can bear loads of 1T-5T and is used as wire rope. This construction is widely used in the North Sea oil industry.
Surface treatment: bright or galvanized
Standard: GB/T 20118-2006
Engineering Applications
Drilling line
Elevator hoisting rope
Wire rope slings
Luffing wire rope
Hoisting rope
Crane wire rope
Sandline, coring line and swabbing line
Trawling / ocean sweeping
Grounding wire rope / ground drag rope
Oil well / oilfield
Excavator rope / scraper rope
Fishing rope
Towing rope
Breaking load
|
|
Minimum breaking load |
Minimum breaking load |
Minimum breaking load | Minimum breaking load |
|---|---|---|---|---|---|
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 14 | 0.7 | 114 | 11677 | 127 | 12930 |
| 16 | 0.92 | 150 | 15252 | 166 | 16889 |
| 18 | 1.16 | 189 | 19303 | 210 | 21375 |
| 20 | 1.44 | 234 | 23831 | 259 | 26389 |
| 22 | 1.74 | 283 | 28835 | 313 | 31931 |
| 24 | 2.07 | 336 | 34317 | 373 | 38000 |
| 26 | 2.43 | 395 | 40274 | 437 | 44598 |
| 28 | 2.82 | 458 | 46709 | 507 | 51723 |
| 30 | 3.23 | 526 | 53620 | 582 | 59376 |
| 32 | 3.68 | 598 | 61008 | 662 | 67556 |
| 34 | 4.15 | 675 | 68872 | 748 | 76265 |
| 36 | 4.65 | 757 | 77213 | 838 | 85501 |
| 38 | 5.18 | 843 | 86030 | 934 | 95265 |
| 40 | 5.74 | 935 | 95325 | 1035 | 105557 |
| 42 | 6.33 | 1030 | 105095 | 1141 | 116377 |
| 44 | 6.95 | 1131 | 115343 | 1252 | 127724 |
| 46 | 7.6 | 1236 | 126067 | 1369 | 139600 |
| 48 | 8.27 | 1346 | 137268 | 1490 | 152003 |
General Engineering Wire Rope
Greenlogy TEC (LM) specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these standard wire ropes, we can also supply premium special wire ropes.
Most wire ropes work under demanding conditions and must be resistant to crushing, bending fatigue and abrasion. All our wire ropes aim to achieve high performance levels to extend service life and thereby improve end-user productivity. We therefore ensure that all materials are produced in accordance with wire rope industry standards. Each wire rope can be supplied with assembly components such as thimbles, swaged ends and wedge sockets, as well as many other fittings. We also offer customization: our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable and comply with ISO9001..
Selection Guide
This product is Greenlogy TEC GB (Coated) Compacted Filler Wire Rope 6X19 (12/6+6F/1) FC construction, with a fiber core, suitable for lifting and hauling applications requiring a degree of flexibility and load capacity. When selecting, we recommend matching based on the working conditions, required diameter, breaking load requirements and surface treatment (bright or galvanized). Contact us for detailed specifications and a quotation, and our technical staff will assist in confirming the suitable model.
Product Advantages
This wire rope adopts a compacted filler construction, balancing flexibility and abrasion resistance while ensuring breaking load, and its surface can be bright or galvanized to suit different environments. It complies with the GB/T 20118-2006 standard and is commonly used in drilling lines, elevator hoist ropes, slings and lifting, among many other engineering applications. Contact us to learn about specific advantages and suitable solutions.
Inquiry Guide
For specific diameter, weight, corresponding breaking load parameters and surface treatment options of this product, please contact us for detailed specifications and a quotation. Please provide information such as the application, required diameter and quantity, and we will recommend suitable specifications based on your needs and assist with selection.
Operating Environment
- The fiber core (FC) in this compacted 6X19 wire rope requires a dry, indoor environment; when used in the North Sea oil industry, moisture ingress must be prevented.
- The galvanized surface treatment option provides corrosion resistance for outdoor applications, such as trawling, ocean sweeping, and grounding wire rope.
- As a drilling line, elevator hoisting rope, and crane wire rope, this product may operate in industrial settings with exposure to dust, humidity, and varying temperatures, where the bright finish offers no additional corrosion protection.
- In luffing and hoisting applications, the rope's performance can be affected by corrosive media; regular inspection and maintenance are recommended.