Product Category

LM (Coating) Comp. Non-rotating Wire Rope GB37X7 (6/1)


Contact us for a quotation

Product details

Product Details

37x7 (coated) wire rope is available in both galvanized and non-galvanized options. Based on your requirements for higher breaking load and better wear characteristics, we can apply surface treatment, lubrication, plastic coating, and compaction.

Surface treatment: bright or galvanized

Standard: GB/T 20118-2006

Engineering Applications 

  • Offshore crane wire rope

  • Deck crane wire rope

  • Pillar crane wire rope

  • Lifting slings

  • Main hoist wire rope

  • Sling

Breaking load

Minimum breaking load

Minimum breaking load

Minimum breaking load

Minimum breaking load


Weight

Weight

(1770Mpa)

(1770Mpa)

(1960Mpa)

(1960Mpa)

mm

kg/m

KN

Kg

KN

Kg

140.951541570817117442
151.091771805419619992
161.252032070622522950
181.582572621428529070
191.782902958032132742
201.953183243635235904
212.153493559838739474
222.373853927042643452
232.564164243246147022
242.814574660150651612
253.15045151055856916
263.35375477459560690
283.86186303668569870
294.16676803473875276
304.457247384880281804
324.968068221289290984

General engineering wire rope

   Greenlogy TEC (LM) specializes in supplying multi-strand bright or galvanized wire rope. Our products range from 0.5 mm to 64 mm in diameter, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these standard wire ropes, we can also supply premium special wire ropes.

Most wire ropes operate under demanding conditions and must resist crushing, bending fatigue and wear. All our wire ropes are engineered to achieve a high performance level to extend service life and thereby improve end-user productivity. We therefore ensure all materials are produced in accordance with wire rope industry standards. Each wire rope can be supplied with fittings such as thimbles, swaged terminals and wedge sockets as well as many other assembly components. We also offer customization services; our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable and compliant with ISO9001.


Selection Guide

This product is an LM (coated) compacted non-rotating wire rope with a construction of GB37X7 (6/1), suitable for lifting and hoisting applications requiring non-rotating performance and wear resistance. When selecting, please consider the working load limit, sheave and drum diameters, frequency of use and corrosive environment of the application to confirm the required diameter and surface treatment (bright or galvanized). As this page does not list the full specification coverage, please contact us for detailed specifications and selection advice.

Product Advantages

This construction features non-rotating characteristics, and the coating helps improve wear resistance and corrosion protection. It can also be adjusted through processes such as surface treatment, lubrication, plastic coating or compaction as required. The choice of galvanized and non-galvanized options makes it easy to match different corrosion levels, suitable for applications such as offshore cranes, deck cranes, pillar cranes, lifting slings and main hoists. Specific performance varies with diameter, construction and process. Please contact us for detailed technical data and quotations.

Inquiry Guidance

To confirm the suitable diameter, surface treatment method, coating or plastic sheathing requirements, as well as bulk supply and delivery arrangements, please provide your operating parameters and required quantity. You are welcome to contact us for detailed specifications, samples and quotations; we will provide targeted recommendations based on your application scenario.

Operating Environment

  • The LM (Coating) 37x7 (6/1) non-rotating wire rope is suited to outdoor marine and offshore working conditions, where it is exposed to salt-laden air and repeated wetting on deck cranes, pillar cranes and offshore crane installations.
  • The galvanized or bright surface treatment is selected according to the corrosivity of the site, and the coating, lubrication, plastic coating and compaction options help the rope resist abrasion and moisture in humid or splash-zone service.
  • Typical uses such as main hoist ropes, lifting slings and sling assemblies place the rope in continuously loaded, dust- and dirt-exposed industrial surroundings where wear resistance is required.
  • For guidance on storage, temperature range and suitability for a specific corrosive medium, contact the supplier with the details of your application.