Genius FRP  

  Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.  

Name

Contect

Type

Resin

25%

OFR-25,IFR-25,VEFR-25

Fiberglass

65%

E

Filler

8%

ATH,PR

Others

2%

---

Introduction of raw materials 
Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Sand surface

Software - Sample 2 for three columns

Smooth surface

Software - Sample 3 for three columns

Antiskid groove surface

I 5010

Standard Panel Size:
1220mm,915mm-wide  3050mm,6100mm-length
Bearing Bar: 25mm
Open Area: 50%
Approx Weight (With three-core shoots): 15.1kg/m²
Liner load

Liner load(units:mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Limit

(mm)

300450750150030005950

Load

4500.460.711.172.334.668.5213808
6001.111.652.745.8311.218.810799
9003.545.068.8616.534.959.27194
12008.3712.922.239.6------5362
Uniform load

Uniform load(units:mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Limit

(mm)

1000190039007000950019500

Load

4500.911.763.275.549.3215.660499
6002.154.299.0615.11826.535429
9007.8312.923.7---------15638
120017.5---------------8796

The characteristics:

  • Fire Retardant

  • High Flame Resistance

  • Low Smoke and Toxic Fume Emissions

  • High Strength-to-Weight Ratio

  • Corrosion Resistant

  • Low Maintenance

  • Slip Resistant

  • Electrically & Thermally Non-Conductive

  • Easily Fabricated

  • Impact Resistant 

  • UV resistance

  • Maintenance free

Installation and accessories  

I 5010

Application Scenarios

Pultruded Grating I-5010 is suitable for industrial platforms, walkways, stair treads, trench covers and similar applications requiring corrosion resistance, light weight and high strength. Its structural type is also commonly used in wastewater treatment, chemical engineering, marine engineering and other environments with moisture or chemical media. To learn about its suitability under specific working conditions, please contact us for detailed specifications and a quotation.

Selection Guide

Selection requires comprehensive consideration of load requirements, span, service environment and installation method. This product uses pultruded I-profiles as bearing bars and solid tubes or rods as connecting rods. Different resin systems (such as orthophthalic, isophthalic, vinyl ester, etc.) can be selected according to actual needs to meet corrosion resistance or flame retardant requirements. Please contact us for detailed specifications and a quotation, and we will assist you in completing the selection.

Product Advantages

Pultruded Grating I-5010 features light weight, high strength, corrosion resistance, slip resistance and insulation properties, and is easy to cut and install. Its structural design effectively reduces overall weight while maintaining load-bearing capacity, making it suitable for applications sensitive to self-weight or requiring frequent disassembly. Please contact us for detailed specifications and a quotation to learn more about product advantages.

Inquiry Guide

To obtain detailed technical parameters, samples or a quotation for Pultruded Grating I-5010, please contact us via the website contact information. We can provide customized solutions according to your specific application requirements. Please contact us for detailed specifications and a quotation.

Operating Environment

  • Pultruded FRP grating I-5010 is built around pultruded I-shaped bearing bars and solid pipe or bar connecting rods, so it is intended for indoor and outdoor service where the grating stays exposed to weather, moisture and temperature swings.
  • The resin system selected for the bearing bars — phenolic type or vinyl type, with the flame-retardant properties listed above — determines how the grating behaves in humid, chemically aggressive or fire-sensitive surroundings, so the resin grade should be matched to the actual working atmosphere.
  • Because the bearing bars and connecting rods are pultruded FRP rather than steel, the grating line is normally chosen for walkways, platforms and similar access areas in corrosive or wet industrial settings where a rust-prone surface would be a maintenance concern.
  • For the exact temperature range, chemical resistance data and suitable service conditions of a given resin grade, contact us with the intended installation environment so the correct configuration can be confirmed.

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。

发送