Genius FRP  

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

38 38 50 Heavy duty

38*38*50(mm)

Panel size available:

1220*4000,1220*3660,1220*2440,

915*3050 Bidirectional force.

Bearing bar thickness (Top/Bottom):11/9.0

Bearing bar center:38

Open Aera:56%

Approx Weight:42kgs/m²

Liner load

Liner load(units:mm)

 Span in (mm)

Load in kn/m of widht (concentrated)

Maximum

Recommended

Apparent E1*10^6 N-mm^2/m

4009.3197.14
Uniform load

Uniform load(units:mm)

 Span in (mm)

Load in kn/sqm (uniformed)

Maximum

Recommended

Apparent E1*10^6 N-mm^2/m

4002.31007.14
6009.9458.55
38 38 50 Heavy duty

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

38 38 50 Heavy duty
38 38 50 Heavy duty
38 38 50 Heavy duty

Application Scenarios

Greenlogy TEC FRP molded grating 38*38 H50 heavy-duty type is suitable for operating platforms, walkways, trench covers and other applications requiring high load-bearing capacity and corrosion resistance in petrochemical, power, wastewater treatment, marine engineering and other industries.

Its 38*38mm mesh and 50mm thickness design provides high strength while maintaining drainage, anti-slip and ventilation performance, making it suitable for humid environments, areas prone to liquid accumulation, or places requiring frequent washing.

Selection Guide

When selecting, load-bearing requirements, span, support method and service environment should be comprehensively considered, and appropriate thickness and mesh size should be selected according to actual loads.

If a higher corrosion resistance grade is required, isophthalic, vinyl ester or bisphenol A resins can be selected; when flame retardant performance is needed, formulations with added flame retardants are available. Please contact us for detailed specifications and selection advice.

Product Advantages

This product uses unsaturated polyester resin as the matrix and is reinforced with glass fiber, featuring lightweight and high strength, corrosion resistance, aging resistance, insulation and maintenance-free properties.

The molding process ensures accurate mesh dimensions and good integrity, the surface groove design provides anti-slip effect, and the heavy-duty structure can withstand relatively large concentrated loads.

Inquiry Guide

For more information on the technical parameters, customized sizes or bulk purchase of Greenlogy TEC FRP molded grating 38*38 H50 heavy-duty type, please contact us for detailed specifications and quotations.

We can provide selection support and solutions according to your specific needs. Please feel free to contact us.

Operating Environment

  • Molded FRP grating with 38×38 mm mesh and 50 mm depth is built for heavy-load service in industrial plants, walkways, platforms and stair treads where steel grating would corrode.
  • The isophthalic, vinyl ester and bisphenol unsaturated polyester resin systems named in the raw-material table suit outdoor and indoor exposure to moisture, humidity and chemical splash; the phenolic grade is offered where fire safety and low toxicity are required.
  • Because the load-bearing structure is molded from resin, E-glass fiber and ATH or PR filler rather than welded metal, the grating performs in corrosive and wet atmospheres where periodic washdown is normal.
  • For temperature limits, chemical resistance ratings against specific media and the full parameter list, contact Greenlogy TEC with your service conditions.

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。

发送