玻璃钢模塑格栅25*100H25标准负载型

玻璃钢模塑格栅25*100H25标准负载型

价格面议

发起询价


欢迎询价。

Genius FRP     

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

 Resin type  

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasio

Selected filler type   

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type

Software - Sample 2 for three columns

Polished type

Software - Sample 3 for three columns

Shop sand type

25 100 H25 Standard duty

25*100*25(mm)

Panel size available:

1220*3660 Length stress\Width stress 

Bearing bar thickness (Top/Bottom):6.5/5.0

Bearing bar center:25

Open Aera:67%

Approx Weight:13.83kgs/m²

25 100 H25 Standard duty

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

Software - Sample 1 for three columns
Software - Sample 2 for three columns
Software - Sample 3 for three columns

Application Scenarios

FRP molded grating 25*100 H25 standard load type is suitable for general industrial platforms, walkways, trench covers and equipment operating surfaces where slip resistance, corrosion resistance and moderate load-bearing capacity are required. In chemical, water treatment, electroplating and other environments with certain corrosive media, this specification can serve as one of the common options; for specific suitability, please contact us to confirm based on your actual working conditions.

Selection Guide

During selection, the resin system, grating thickness and mesh size can be matched to the corrosion level and load requirements of the service environment: the 25mm thick, 100mm mesh specification focuses on standard load and routine slip resistance. If special media, high temperature or higher load-bearing requirements are involved, we recommend providing working condition parameters, and we can assist in recommending a more suitable resin type and structural solution; please contact us for detailed specifications and quotations.

Product Advantages

This molded grating is integrally formed from unsaturated polyester resin and E-glass fiber in a custom mold, possessing the common characteristics of FRP materials such as light weight, high strength, corrosion resistance, slip resistance and insulation. The molding process enables continuous fibers to be distributed in both the longitudinal and transverse directions, giving good impact resistance and integrity, while also being easy to cut and install, helping to reduce subsequent maintenance workload.

Inquiry Guide

If you need to know the specifications and parameters, resin selection or supply information for FRP molded grating 25*100 H25 standard load type, please contact us for detailed specifications and quotations. We will provide targeted product recommendations and technical support based on your actual application scenarios.

Operating Environment

  • This FRP molded grating is built on unsaturated polyester resin, so it is typically specified for industrial settings where continuous or intermittent contact with corrosive media such as acids, alkalis and salts would shorten the life of conventional metal gratings.
  • The molded open-grid structure makes the grating suitable for both indoor plant areas and outdoor installations, including walkways, platforms and trench covers that are exposed to sunlight, rain and wash-down.
  • Because the resin system can be selected from isophthalic, vinyl ester or bisphenol types, the grating is commonly used in chemical, wastewater and marine-adjacent environments where humidity and chemical splash are part of normal operation.
  • Service temperature and chemical resistance vary with the chosen resin grade; contact us for the suitable resin type and the full parameter list for your specific operating conditions.