结构型材-七孔空心板(间苯)

结构型材-七孔空心板(间苯)

价格面议

发起询价


欢迎询价。

Genius FRP  

   FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.   

Seven hole hollow board

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)


600*8.5*56*825.4

24" x 5/16" x 2" x 5/16"

56

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

 Application:  

   Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.  

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

The seven-hole hollow plate (isophthalic) is suitable for structural and load-bearing locations requiring strength, span and corrosion resistance, such as building platforms, bridge and tunnel components, support structures in chemical and food processing environments, and walkways and frames at manufacturing and mining sites. If you need to confirm a usage scheme based on specific working conditions, please contact us to obtain detailed specifications and a quotation.

Selection Guidance

During selection, you may start from conditions such as load-bearing requirements, span, support spacing, service environment and installation method, and judge in combination with how well the isophthalic resin system matches properties such as corrosion resistance. Please inform us of your drawings or working condition parameters so that we can assist in confirming suitable specifications and configuration.

Product Advantages

This structural profile uses glass fiber reinforced material and resin as its matrix, and is formed through impregnation, hot press curing and pultrusion. It has good physical properties, is suitable for high-strength and large-span use scenarios, and is easy to cut and install on site. The above content covers general product characteristics; for specific performance data, please refer to the technical materials we provide. Please contact us to obtain detailed specifications and a quotation.

Inquiry Guidance

If you need information on the specifications, performance or supply of Structural Profile - Seven-Hole Hollow Plate (Isophthalic), please contact us and state the application scenario and required quantity, and we will provide corresponding technical support and commercial solutions accordingly. Please contact us to obtain detailed specifications and a quotation.

Operating Environment

  • FRP structural shapes profile resists corrosion from acids, alkalis and salts, making it suitable for chemical processing, food and beverage plants, and other facilities where moisture or aggressive media are present.
  • The glass fiber reinforced composite construction withstands outdoor exposure, including UV radiation and temperature fluctuations, for applications in architectural, bridge and highway, and metals and mining environments.
  • With low thermal conductivity, the profiles help reduce heat transfer in high-humidity or condensing conditions, supporting use in microelectronics and manufacturing settings where stable performance is required.
  • FRP structural shapes profile is non‑magnetic and non‑sparking, allowing safe operation near sensitive equipment or in environments where metallic materials may pose a risk.