结构型材-踢脚板 (邻苯)

结构型材-踢脚板 (邻苯)

价格面议

发起询价


欢迎询价。

Genius FRP   

  FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

Skirting board

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Skirting board

A*B*T


A*B*T


M2

100*13*3.2 M-shape

1.1

4" x 1/2" x 1/8" M-shape

2.43

M3

100*16*5 M-shape

1.3

4" x 5/8" x 3/16" M-shape

2.87

M4

148*12*3 M-shape

1.27

23/4" x 1/2" x 1/8" M-shape

2.8

W1

100*19*5 W-shape

1.36

4" x 3/4" x 3/16" W-shape

3

W2

100*15*3.2 W-shape

1.1

4" x 9/16" x 1/8" W-shape

2.43

W3

150*15*3.2 W-shape

1.6

6" x 9/16" x 1/8" W-shape

3.53

Markets  

Markets
  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

  Application:  

   Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.   

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

Kick plate profiles are suitable for protection and decorative edging on industrial platforms, floor edges and in corrosive environments, and can be used with structural profile systems. In chemical plants, wastewater treatment and marine engineering applications, they provide corrosion-resistant, insulating kick plate protection and extend the service life of the base structure. Contact us to learn about specific application cases and matching solutions.

Selection Guide

Please select the cross-section shape and thickness according to the dimensions of the installation location, load-bearing requirements and environmental conditions; models such as M2, M3 and M4 correspond to different sizes. If you need custom lengths or colors, provide drawings or samples and we will assist with selection. Contact us for detailed specification sheets and technical support.

Product Advantages

FRP kick plates feature light weight, high strength, corrosion resistance, insulation and low maintenance, with a smooth, easy-to-clean surface and strong design flexibility. Compared with traditional metal materials, they last longer in humid or chemically corrosive environments and are easy to install. Contact us for samples and performance data.

Inquiry Guide

To obtain product quotations, technical parameters or customized services, please contact us through the website and provide the required model, quantity and application, and we will reply as soon as possible. You are welcome to inquire about cooperation.

Operating Environment

  • FRP skirting boards are suitable for both indoor and outdoor installations, including industrial plants, walkways, and platforms.
  • The glass fiber reinforced composite construction provides resistance to moisture and humidity, making it appropriate for use in damp or wet environments.
  • These profiles withstand exposure to many corrosive media encountered in industrial settings, such as chemical plants and wastewater treatment facilities.
  • They perform reliably across a range of ambient temperatures typical of industrial and commercial applications.

立即联系我们,我们将有专业人员为您服务。