 Genius FRP

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

 Resin type  

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

38*38H30 Heavy duty

38*38*30(mm)

Panel size available:

1220*3660,1220*2440,915*3050

Bidirectional force. 

Bearing bar thickness (Top/Bottom):10.5/9.0

Bearing bar center:38

Open Aera:56% 

Approx Weight:25kgs/㎡ 

Liner load

Liner load(units:mm) 

Deflcvtion



kg/m




Limit

Span
(mm)

150

300

450

600

750

1500

Load

3000.360.480.610.760.891.0617116
6000.661.251.852.463.078.488718
9001.803.685.567.429.3013.85817
12004.759.6814.619.621.2---3755
Uniform load

Uniform load(units:mm)

Deflcvtion



kg/m²




Span
(mm)

240

480

980

1450

2450

3650

4880

3000.090.190.380.490.781.05---
6000.430.811.552.313.845.74---
9001.703.456.9610.4717.523.3---
12005.9712.224.532.638.7------
Software image and text block

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly. 

38*38H30 Heavy duty
38*38H30 Heavy duty
38*38H30 Heavy duty

Application Scenarios

FRP molded grating 38×38 H30 heavy-duty type is suitable for industrial platforms, walkways, trench covers and equipment operating surfaces that require relatively high load-bearing capacity and corrosion resistance. Its grid structure and resin system can adapt to environments with moisture or corrosive media in chemical, water treatment, power and other industries. For specific suitability, we recommend confirming with us based on your operating conditions.

Selection Guide

When selecting, please consider load-bearing requirements, support span, type of corrosive media and installation method, and match them with the resin system and grating thickness. This product is a heavy-duty molded grating with 38×38 mm mesh and 30 mm thickness. If you need to compare selections under different load conditions, please contact us for detailed specifications and technical support.

Product Advantages

Molded grating is integrally formed from resin and fiberglass, featuring light weight, high strength, corrosion resistance, slip resistance and insulation, and is easy to cut and install. The heavy-duty structure improves load-bearing performance while maintaining open area, making it suitable for applications with requirements for strength and durability.

Inquiry Guide

If you would like to know the detailed specifications, resin system options and commercial terms of FRP molded grating 38×38 H30 heavy-duty type, please contact us for specifications and a quotation. We will provide a suitable solution based on your project requirements.

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。

发送