Genius FRP  

  Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.  

Name

Contect

Type

Resin

25%

OFR-25,IFR-25,VEFR-25

Fiberglass

65%

E

Filler

8%

ATH,PR

Others

2%

---

Introduction of raw materials 
Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Sand surface

Smooth surface

Antiskid groove surface

Standard Panel Size:
1220mm,915mm-wide  3050mm,6100mm-length
Bearing Bar: 25mm
Open Area: 60%
Approx Weight (With three-core shoots): 12.2kg/m²

Liner load(units:mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Limit

(mm)

300450750150030005950

Load

4500.590.891.522.945.831111067
6001.412.123.525.5914.227.68639
9004.757.13
11.923.7------5750
120011.216.928.2---------4275

Uniform load(units:mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Limit

(mm)

1000190040007000950019500

Load

4501.232.364.958.6711.922.248380
6002.935.3511.7---------28344
9009.9119.52------------12559
120023.5---------------6988

The characteristics:

  • Fire Retardant

  • High Flame Resistance

  • Low Smoke and Toxic Fume Emissions

  • High Strength-to-Weight Ratio

  • Corrosion Resistant

  • Low Maintenance

  • Slip Resistant

  • Electrically & Thermally Non-Conductive

  • Easily Fabricated

  • Impact Resistant 

  • UV resistance

  • Maintenance free

Installation and accessories  


Application Scenarios

Pultruded Grating I-6010 is suitable for platforms, walkways, trench covers and various industrial operating surfaces that require both load-bearing capacity and corrosion resistance. Its structure uses pultruded "I" profiles as load-bearing bars and solid tubes or rods as connecting rods, helping it remain stable in humid, chemically aggressive or outdoor environments. For specific application matching and installation methods, please contact us to confirm based on your operating conditions.

Selection Guide

When selecting, first clarify the corrosive media and fire protection requirements of the service environment, then choose the resin system accordingly. For example, phenolic type is suitable for applications with low toxicity, high flame retardancy and high fire safety requirements, while vinyl ester type is suitable for general corrosion-resistant conditions. At the same time, consider the grating's load-bearing direction, support span and installation fixing method. We can assist you with selection; please provide operating condition parameters to receive recommendations.

Product Advantages

Pultruded Grating I-6010 is made from fiberglass and resin systems and formed by a profile assembly process. It combines light weight, high strength, corrosion resistance and ease of cutting and installation. The surface can be treated for anti-slip performance according to use requirements, and the combined structure of connecting rods and load-bearing bars helps distribute loads. Compared with traditional metal gratings, it offers advantages in chemical corrosion resistance and insulation.

Inquiry Guidance

To obtain detailed specifications, resin type options, load-bearing data and commercial terms for Pultruded Grating I-6010, please contact our sales team. Please provide your application environment, size requirements and quantity, and we will provide a targeted solution and quotation.