Genius FRP
Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
|---|---|---|
Resin |
25% | OFR-25,IFR-25,VEFR-25 |
Fiberglass |
65% | E |
Filler | 8%
| ATH,PR |
Others |
2% | --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |

Sand surface

Smooth surface

Antiskid groove surface

Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 25mm
Open Area: 60%
Approx Weight (With three-core shoots): 12.2kg/m²

Liner load(units:mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 300 | 450 | 750 | 1500 | 3000 | 5950 | Load |
| 450 | 0.59 | 0.89 | 1.52 | 2.94 | 5.83 | 11 | 11067 |
| 600 | 1.41 | 2.12 | 3.52 | 5.59 | 14.2 | 27.6 | 8639 |
| 900 | 4.75 | 7.13 | 11.9 | 23.7 | --- | --- | 5750 |
| 1200 | 11.2 | 16.9 | 28.2 | --- | --- | --- | 4275 |

Uniform load(units:mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 1000 | 1900 | 4000 | 7000 | 9500 | 19500 | Load |
| 450 | 1.23 | 2.36 | 4.95 | 8.67 | 11.9 | 22.2 | 48380 |
| 600 | 2.93 | 5.35 | 11.7 | --- | --- | --- | 28344 |
| 900 | 9.91 | 19.52 | --- | --- | --- | --- | 12559 |
| 1200 | 23.5 | --- | --- | --- | --- | --- | 6988 |
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories

Application Scenarios
Pultruded Grating I-6010 is suitable for platforms, walkways, trench covers and various industrial operating surfaces that require both load-bearing capacity and corrosion resistance. Its structure uses pultruded "I" profiles as load-bearing bars and solid tubes or rods as connecting rods, helping it remain stable in humid, chemically aggressive or outdoor environments. For specific application matching and installation methods, please contact us to confirm based on your operating conditions.
Selection Guide
When selecting, first clarify the corrosive media and fire protection requirements of the service environment, then choose the resin system accordingly. For example, phenolic type is suitable for applications with low toxicity, high flame retardancy and high fire safety requirements, while vinyl ester type is suitable for general corrosion-resistant conditions. At the same time, consider the grating's load-bearing direction, support span and installation fixing method. We can assist you with selection; please provide operating condition parameters to receive recommendations.
Product Advantages
Pultruded Grating I-6010 is made from fiberglass and resin systems and formed by a profile assembly process. It combines light weight, high strength, corrosion resistance and ease of cutting and installation. The surface can be treated for anti-slip performance according to use requirements, and the combined structure of connecting rods and load-bearing bars helps distribute loads. Compared with traditional metal gratings, it offers advantages in chemical corrosion resistance and insulation.
Inquiry Guidance
To obtain detailed specifications, resin type options, load-bearing data and commercial terms for Pultruded Grating I-6010, please contact our sales team. Please provide your application environment, size requirements and quantity, and we will provide a targeted solution and quotation.