Product Category

玻璃钢模塑格栅38*38H35 重负载型


Contact us for a quotation

产品详情

Genius FRP  

 Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.  

Name

Contect

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials 
resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

VEFR-10

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type   

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Groove type

Polished type

Shop sand type

38*38*35(mm)

Panel size available: 

1220*3660,1220*2440,915*3050 

Bidirectional force. 

Bearing bar thickness (Top/Bottom):10.5/9.0 

Bearing bar center:38

Open Aera:56% 

Approx Weight:29.4kgs/㎡ 

Liner load(units:mm)

 Span in (mm)

Load in kn/m of widht (concentrated)

Maximum

Recommended

Apparent E1*10^6 N-mm^2/m

4007.3197.14

Uniform load(units:mm)

 Span in (mm)

Load in kn/sqm (uniformed)

Maximum

Recommended

Apparent E1*10^6 N-mm^2/m

4001.81007.14
6007.7458.55

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.


Application Scenarios

FRP molded grating 38*38H35 heavy-duty type is suitable for industrial platforms, trench covers, stair treads and equipment walkways that require high load-bearing capacity and corrosion resistance. Its structural design meets the demands of long-term use in heavy-load environments. Specific load-bearing performance should be evaluated based on actual support conditions. Contact us for detailed application recommendations.

Selection Guide

When selecting, please consider factors such as load requirements, support span, type of corrosive media and operating environment temperature. Different resin types (such as orthophthalic, isophthalic, vinyl ester, etc.) have different effects on corrosion resistance and flame retardant performance, and can be selected according to specific working conditions. For professional selection support, contact us with your working condition parameters for targeted recommendations.

Product Advantages

This grating is manufactured by a molded process and features light weight, high strength, corrosion resistance, slip resistance and insulation, and is easy to cut and install. The heavy-duty design enhances load-bearing capacity while maintaining the inherent advantages of FRP materials, making it suitable for structural locations with higher requirements. For specific performance data, please refer to actual test reports. Inquiries are welcome.

Inquiry Guide

For detailed specifications, technical parameters, prices and supply information of FRP molded grating 38*38H35 heavy-duty type, please contact us. Kindly provide your specific application scenario and required quantity, and we will provide a professional response as soon as possible.