玻璃钢模塑格栅38*38H35 重负载型
发起询价
欢迎询价。
Genius FRP
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Contect | Type |
|---|---|---|
Resin | 35% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH,PR |
Others | 1% | --- |
Code | Resin type | Flame retardant property |
Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | VEFR-10 | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




38*38*35(mm)
Panel size available:
1220*3660,1220*2440,915*3050
Bidirectional force.
Bearing bar thickness (Top/Bottom):10.5/9.0
Bearing bar center:38
Open Aera:56%
Approx Weight:29.4kgs/㎡

Liner load(units:mm)
Span in (mm) |
Load in kn/m of widht (concentrated) | Maximum Recommended | Apparent E1*10^6 N-mm^2/m |
| 400 | 7.3 | 19 | 7.14 |

Uniform load(units:mm)
Span in (mm) |
Load in kn/sqm (uniformed) | Maximum Recommended | Apparent E1*10^6 N-mm^2/m |
|---|---|---|---|
| 400 | 1.8 | 100 | 7.14 |
| 600 | 7.7 | 45 | 8.55 |

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.



Application Scenarios
FRP molded grating 38*38H35 heavy-duty type is suitable for industrial platforms, trench covers, stair treads and equipment walkways that require high load-bearing capacity and corrosion resistance. Its structural design meets the demands of long-term use in heavy-load environments. Specific load-bearing performance should be evaluated based on actual support conditions. Contact us for detailed application recommendations.
Selection Guide
When selecting, please consider factors such as load requirements, support span, type of corrosive media and operating environment temperature. Different resin types (such as orthophthalic, isophthalic, vinyl ester, etc.) have different effects on corrosion resistance and flame retardant performance, and can be selected according to specific working conditions. For professional selection support, contact us with your working condition parameters for targeted recommendations.
Product Advantages
This grating is manufactured by a molded process and features light weight, high strength, corrosion resistance, slip resistance and insulation, and is easy to cut and install. The heavy-duty design enhances load-bearing capacity while maintaining the inherent advantages of FRP materials, making it suitable for structural locations with higher requirements. For specific performance data, please refer to actual test reports. Inquiries are welcome.