LM Wire Rope GB 6x37 FC
Please feel freely to contact with us for new price .
Product Details
6x37规格一般用于工程上的交叉铺设,还提供FC(进口麻芯)。6x36在英国更受欢迎;而在欧洲大陆,一般使用6x37规格。
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006

Applications
General engineering applications
Crane ropes
Hoist rope
Breaking Loads
|
|
Min Breaking Loads | Min Breaking Loads |
Min Breaking Loads | Min Breaking Loads |
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 12 | 0.5 | 75.2 | 7669 | 83.3 | 8492 |
| 13 | 0.59 | 88.2 | 9000 | 97.7 | 9967 |
| 14 | 0.68 | 102 | 10438 | 113 | 11559 |
| 16 | 0.89 | 134 | 13634 | 148 | 15098 |
| 18 | 1.12 | 169 | 17256 | 187 | 19108 |
| 20 | 1.38 | 209 | 21303 | 231 | 23590 |
| 22 | 1.68 | 253 | 25777 | 280 | 28544 |
| 24 | 1.99 | 301 | 30677 | 333 | 33970 |
| 26 | 2.34 | 353 | 36003 | 391 | 39868 |
| 28 | 2.71 | 409 | 41755 | 453 | 46237 |
| 30 | 3.11 | 470 | 47933 | 520 | 53078 |
| 32 | 3.54 | 535 | 54537 | 592 | 60391 |
| 34 | 4 | 604 | 61567 | 668 | 68176 |
| 36 | 4.48 | 677 | 69024 | 749 | 76433 |
| 38 | 5 | 754 | 76906 | 835 | 85161 |
| 40 | 5.54 | 835 | 85214 | 925 | 94362 |
| 42 | 6.1 | 921 | 93949 | 1020 | 104034 |
| 44 | 6.7 | 1011 | 103110 | 1119 | 114178 |
| 46 | 7.32 | 1105 | 112696 | 1224 | 124794 |
| 48 | 7.97 | 1203 | 122709 | 1332 | 135881 |
General Engineering Ropes
绿盟LM专门供应多股光面或镀锌钢丝绳。我们的产品直径从0.5mm到64mm不等,包括带纤维芯和钢芯的1X19、7X7、6X19、7X19、6X36、8X19、8X36、19X7和35X7各种规格。除这些常规钢丝绳外,我们还可以提供优质的特种钢丝绳。
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.