Product Category

Structural Profiles - Three-Cell Hollow Profile (Vinyl Ester)


Contact us for a quotation

Product details

Greenlogy TEC

   FRP pultruded profiles are made from glass fiber reinforcement as the raw material, resin as the binder, and glass fiber cloth as the wrapping reinforcement layer. After thorough impregnation, the material is heated, formed and cured in a metal mold and then drawn by a pultrusion machine to produce a new type of composite material with good physical properties, widely used in high-strength and large-span applications.   

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)


450*4.5*150*618.2

18" x 3/16" x 6" x 1/4"

40.1

Markets  

  • Construction

  • Bridges and Highways

  • Chemical

  • Food and Beverage

  • Manufacturing

  • Metals and Mining

  • Microelectronics

  • Oil and Gas

  • Pharmaceutical

  • Power

  • Pulp and Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water and Wastewater Treatment

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Heavy metal resistant

  • Long service life

  • Electrically and thermally non-conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR type: economical, good performance, resistant to moderate acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications: 

   Greenlogy TEC pultruded FRP profiles are widely used in various scenarios, combining corrosion resistance, high strength, dimensional stability and light weight, with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles deliver years of low-maintenance service in applications where steel, aluminum or wood components have traditionally been specified. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.  

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural stress, transverse

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, longitudinal

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, transverse

D-790

10^6psi

0.8

10^6kgf/m²

562

Elastic modulus

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact, longitudinal

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

Max %

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max. 25

Combustibility*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Applications

The three-hole hollow slab (vinyl ester) is suitable for applications with high requirements for corrosion resistance and strength, such as chemical platforms, wastewater treatment facilities, marine engineering, and building structures. Its hollow structure design reduces self-weight while providing good load-bearing capacity, making it suitable for large-span applications. To learn about suitability for specific scenarios, please contact us for detailed specifications and quotations.

Selection Guide

When selecting, factors such as load requirements, span, service environment (corrosiveness, temperature), and installation method should be considered. The vinyl ester resin gives the product excellent corrosion resistance, making it suitable for a variety of chemical environments. Our technical team can assist you in choosing the appropriate specifications based on your specific needs; please contact us for detailed specifications and quotations.

Product Advantages

The three-hole hollow slab is made of glass fiber reinforcement and vinyl ester resin, featuring high strength, light weight, corrosion resistance, insulation, and long service life. Its hollow structure design reduces weight while ensuring mechanical performance, facilitating transportation and installation. The surface is smooth and maintenance costs are low. Please contact us for detailed specifications and quotations.

Inquiry Guidance

If you need detailed technical parameters, custom dimensions, volume pricing, and delivery information for the three-hole hollow slab (vinyl ester), please feel free to contact us. We provide professional technical support and customization services; please contact us for detailed specifications and quotations.

Operating Environment

  • These vinyl ester hollow structural profiles resist corrosion in chemical, food and beverage, and metal and mining plants, where acids, alkalis, salts, and washdown chemicals would attack steel.
  • With a vinyl ester resin matrix and glass fiber reinforcement, these profiles are suitable for outdoor and indoor installations exposed to UV, moisture, and large temperature swings, and will not rust and rot like conventional materials.
  • Their non-conductive and non-magnetic properties make them suitable for microelectronics and manufacturing environments, as well as bridge and highway infrastructure where deicing salts are present.