Product Category

Structural Profiles - Solid Round Rod (Orthophthalic)


Contact us for a quotation

Product details

Greenlogy TEC

  FRP pultruded profiles are a new type of composite material made with glass fiber reinforcement as the base material, resin as the adhesive, and glass fiber cloth as the wrapping reinforcement layer; after thorough impregnation, they are heated, formed and cured in a metal mold and drawn by a pulling machine. They have good physical properties and are widely used in high-strength, long-span applications.  

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Solid Round Rod

D
D
SRR6060.081/4"0.18
SRR959.50.143/8"0.31
SRR12712.70.261/2"0.57
SRR25425.411"2.2
SRR32831.81.515/4"3.33
SRR380382.153/2"4.74
SRR424.20.033/16"0.07
SRR808.00.15/16"0.22
SRR16160.415/8"0.9
SRR19190.553/4"1.21
SRR20200.6213/16"1.37
SRR22220.727/8"1.59

Markets

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Heavy metal safety

  • Long service life

  • Electrical and thermal insulation

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Harsh corrosive environments such as acids and alkalis

IFR-25

Isophthalic type

Oxygen index 28 and above

An economical VEFR product with excellent performance and moderate resistance to acids, alkalis, and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications: 

    Greenlogy TEC pultruded FRP profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability, and light weight, with thermal and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum, or wood components are traditionally specified. Today, these profiles are often used in highly corrosive applications where stainless steel and other expensive components were previously required.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flammability

ASTM

Unit

Value

Tunnel burn test*

E-84

Flame spread

25 max

Combustibility*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = longitudinal, CW = transverse, PF = perpendicular to laminate face

*Applies to ISOFR and VEFR only


Applications

Solid round rods combine high axial strength with corrosion resistance, and are commonly used in chemical platform guardrails, ladder rungs, cable supports and insulating equipment structures where high strength and rust resistance are required. To confirm suitability for a specific corrosive medium or load condition, please contact us for detailed specifications and a quotation.

Selection Guide

When selecting, first confirm the required diameter (metric or the corresponding imperial size), the length to be used and the type of load (tension, compression or bending), then match these with the installation method and connector type. Our technical team can help recommend specifications based on your operating conditions; contact us for detailed specifications and a quotation.

Product Advantages

This product is made of glass fiber reinforcement with a resin matrix, formed by pultrusion. It offers the typical composite properties of light weight and high strength, corrosion resistance, electrical insulation and low maintenance, and is suitable for replacing some metal rods to reduce long-term maintenance costs. Actual performance data depend on the specific specifications; contact us for detailed specifications and a quotation.

Inquiry Guidance

For commercial information such as dimensional tolerances, available lengths, surface condition and packaging, please provide the required specifications, quantity and delivery destination, and we will reply as soon as possible. Contact us for detailed specifications and a quotation.

Operating Environment

  • The solid round rod is a pultruded FRP profile suitable for long-term indoor and outdoor use. As a structural component it resists atmospheric aging, and its appearance and service are not easily affected by sun and rain.
  • In chemical, pharmaceutical, water and wastewater treatment and other environments with acid, alkali and salt corrosive media, the corrosion resistance of the solid round rod allows it to replace metal round rods as supports and connectors.
  • The pultruded solid round rod provides electrical and thermal insulation and can be used as an insulating support rod in microelectronics, power and similar applications.
  • The solid round rod is flame retardant and has a high strength-to-weight ratio, making it suitable for bridges and highways, transportation, metals and mining and other applications with requirements on component weight and safety; for selection in specific environments, please confirm cross-section dimensions and media conditions with us.