Product Category

Structural Profiles - Seven-Hole Hollow Plate (Isophthalic)


Contact us for a quotation

Product details

Greenlogy TEC

   FRP pultruded profiles are made from glass fiber reinforcement as the raw material, resin as the binder, and glass fiber cloth as the wrapping reinforcement layer. After full impregnation, they are heated, formed and cured in a metal mold and pulled out by a pulling machine. This new composite material has good physical properties and is widely used in high-strength, long-span applications.   

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)


600*8.5*56*825.4

24" x 5/16" x 2" x 5/16"

56

Application markets 

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Leisure and recreation

  • Telecommunications

  • Transportation

  • Water and wastewater

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Safe for contact with heavy metals

  • Long service life

  • Non-conductive and thermally non-conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR type: economical, with good performance, resistant to moderate acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications:  

   Greenlogy TEC pultruded FRP profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today, these profiles are commonly used in highly corrosive environments that previously required stainless steel and other costly components.  

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural stress, transverse

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, longitudinal

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, transverse

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

Maximum %

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flammability

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Maximum 25

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate face

*Applies to ISOFR and VEFR only


Application scenarios

The seven-hole hollow profile (isophthalic) is suitable for structural and load-bearing locations requiring strength, span and corrosion resistance, such as building platforms, bridge and tunnel components, support structures in chemical and food processing environments, and walkways and frames on manufacturing and mining sites. To confirm a solution for your specific operating conditions, contact us for detailed specifications and a quotation.

Selection guidance

When selecting, start from conditions such as load requirements, span, support spacing, service environment and installation method, and judge how well the isophthalic resin system matches the required corrosion resistance and other properties. Please share your drawings or operating parameters with us so we can help confirm suitable specifications and configuration.

Product advantages

This structural profile uses glass fiber reinforcement and resin as its matrix, formed through impregnation, heated compression molding and curing, and pultrusion. It offers good physical properties, is suitable for high-strength and long-span applications, and is easy to cut and install on site. The above describes general product characteristics; for specific performance data, refer to the technical documentation we provide. Contact us for detailed specifications and a quotation.

Inquiry guidance

To learn about specifications, performance or supply information for the structural profile - seven-hole hollow profile (isophthalic), please contact us and state your application and required quantity. We will provide corresponding technical support and a commercial proposal. Contact us for detailed specifications and a quotation.

Service environment

  • FRP profiles resist attack by acids, alkalis and salts, making them suitable for chemical and food and beverage plants and other locations with moisture or corrosive media.
  • The glass fiber reinforced composite structure withstands outdoor exposure, including UV radiation and temperature fluctuations, and is suitable for buildings, bridges and highways, and metal and mining environments.
  • FRP profiles have low thermal conductivity, helping reduce heat transfer under moist or condensing conditions, and are suitable for microelectronics and manufacturing environments requiring stable performance.
  • FRP profiles are non-magnetic and do not spark, so they can be used safely near sensitive equipment or in environments where metal materials may pose a risk.