Structural Profiles - Kick Plates (Orthophthalic)
Product details
Greenlogy TEC
FRP structural profiles are made from glass fiber reinforcing material, with resin as the binder and glass fiber cloth as the wrapping reinforcement layer. After thorough impregnation, the material is heated, shaped and cured in a metal mold and then pultruded under the pull of a traction machine, forming a new type of composite material with good physical properties that is widely used in high-strength, long-span applications.
Variety | Size (mm) | Weight (kg/m) | Size (in) | Weight (lbs/in) |
|---|---|---|---|---|
Kick Plate | A*B*T | A*B*T | ||
M2 | 100*13*3.2 M型 | 1.1 | 4" x 1/2" x 1/8" M型
| 2.43 |
M3 | 100*16*5 M型 | 1.3 | 4" x 5/8" x 3/16" M型 | 2.87 |
M4 | 148*12*3 M型 | 1.27 | 23/4" x 1/2" x 1/8" M型 | 2.8 |
W1 | 100*19*5 W型 | 1.36 | 4" x 3/4" x 3/16" W型 | 3 |
W2 | 100*15*3.2 W型 | 1.1 | 4" x 9/16" x 1/8" W型 | 2.43 |
W3 | 150*15*3.2 W型 | 1.6 | 6" x 9/16" x 1/8" W型 | 3.53 |
Markets
Construction
Bridges and highways
Chemical
Food and beverage
Manufacturing
Metals and mining
Microelectronics
Oil and gas
Pharmaceutical
Power
Pulp and paper
Recreation and entertainment
Telecommunications
Transportation
Water and wastewater treatment
Features:
Corrosion resistant
Low maintenance cost
Flame retardant
Low installation cost
Heavy-metal safe
Long service life
Non-conductive and non-thermal-conductive
High strength-to-weight ratio
Raw material introduction — resin types
Code | Resin type | Flame retardancy | Recommended applications |
|---|---|---|---|
VEFR-25 | Vinyl ester type | Oxygen index 28 and above | Harsh corrosive environments such as acids and alkalis |
IFR-25 | Isophthalic type | Oxygen index 28 and above | VEFR type: economical yet high-performing, suitable for medium acid, alkali and solvent environments |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | General acid and alkali environments |
Applications:
Greenlogy TEC pultruded FRP structural profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight, with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components have traditionally been specified. Today, these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.
Greenlogy TEC profiles
Mechanical Properties | ASTM | Unit | Value | Unit | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short-Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact, LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact, CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excluding Round Rods and Square Rods
Physical Properties | ASTM | Unit | Value |
|---|---|---|---|
Barcol hardness | D-495 | --- | 45 |
24-hour water absorption | D-570 | % max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of thermal expansion, LW | D-696 | 10^-6in./in./℃ | 8 |
Flame retardancy | ASTM | Unit | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame spread | Max. 25 |
Combustibility* | D-635 | --- | Non-combustible |
Electrical properties | ASTM | Unit | Value |
|---|---|---|---|
Arc resistance, LW | D-495 | 秒(s) | 120 |
Dielectric strength, LW | D-149 | kv./in. | 35 |
Dielectric strength, PF | D-149 | Volts/mil | 200 |
Dielectric constant, PF | D-150 | @60hz | 5 |
LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface
*Applies to ISOFR and VEFR only
Applications
Kick plate profiles are suitable for industrial platforms, floor edges, and protective and decorative edge finishing in corrosive environments, and can be used together with structural profile systems. In chemical plants, wastewater treatment facilities, marine engineering and similar locations, they provide corrosion-resistant, insulating kick protection and extend the service life of the base structure. Contact us to learn about specific application cases and suitable solutions.
Selection Guide
Please select the cross-section shape and thickness according to the dimensions of the installation location, load requirements and environmental conditions; for example, models such as M2, M3 and M4 correspond to different sizes. If custom lengths or colors are required, you can provide drawings or samples, and we will assist with selection. Contact us for detailed specification sheets and technical support.
Product Advantages
FRP kick plates feature light weight, high strength, corrosion resistance, insulation and low maintenance; their smooth surface is easy to clean, and they offer wide design flexibility. Compared with traditional metal materials, they last longer in damp or chemically corrosive environments and are easy to install. Contact us for samples and performance data.
Inquiry Guidance
To obtain product quotations, technical parameters or customization services, please contact us through the website and provide the required model, quantity and application; we will reply as soon as possible. We welcome your inquiries and cooperation.
Operating Environment
- FRP kick plates are suitable for indoor and outdoor installation, including industrial plants, walkways and platforms.
- The fiberglass-reinforced composite structure offers moisture and humidity resistance, making it suitable for use in damp or water-immersed environments.
- These profiles can withstand a variety of corrosive media encountered in industrial environments, such as chemical plants and wastewater treatment facilities.
- They can operate reliably across the range of ambient temperatures commonly found in industrial and commercial applications.