Structural Profiles - I-Beam (Orthophthalic)
Product details
Nantong Greenlogy TEC Electronic Technology Co., Ltd.
Pultruded FRP profiles are a new type of composite material made with glass fiber reinforcement as the reinforcing body and resin as the binder, with glass fiber cloth as the wrapping reinforcing layer; after thorough impregnation, the material is heated, formed and cured in a metal die and then pulled by a pulling machine. With good physical properties, they are widely used in high-strength, long-span applications.
Type | Specification (mm) | Weight (kg/m) | Specification (in) | Weight (lbs/in) |
|---|---|---|---|---|
I-beam | A*B*T1*T2 | A*B*T1*T2 | ||
IB32 | 15*32*6.4*4 | 0.51 | 9/16" x 5/4" x 1/4" x 3/16" | 1.12 |
IB38A | 30*38*3*3 | 0.53 | 19/16" x 3/2" x 1/8" x 1/8" | 1.17 |
IB45A | 45*9*180*12 | 5.4 | 7/4" x 3/8" x 7" x 1/2" | 11.9 |
IB50A | 50*102*6.4*6.4 | 2.4 | 2" x 4" x 1/4" x 1/4" | 5.29 |
IB50B | 50*102*8*8 | 3 | 2" x 4" x 5/16" x 5/16" | 6.61 |
IB76A | 76*152*6.4*6.4 | 3.59 | 3" x 6" x 1/4" x 1/4" | 7.91 |
IB76B | 76*152*9.5*9.5 | 5.32 | 3" x 6" x 3/8" x 3/8" | 11.73 |
IB102A | 102*203*9.5*9.5 | 7.2 | 4" x 8" x 3/8" x 3/8" | 15.87 |
IB102B | 102*203*12.7*12.7 | 9.5 | 4" x 8" x 1/2" x 1/2" | 20.94 |
IB120 | 120*240*12*12 | 10.5 | 19/4" x 19/2" x 1/2" x 1/2" | 23.15 |
IB127A | 127*254*9.5*9.5 | 9 | 5" x 10" x 3/8" x 3/8" | 19.84 |
IB127B | 127*254*12.7*12.7 | 11.9 | 5" x 10" x 1/2" x 1/2" | 26.24 |
IB127C | 127*152*9.5*9.5 | 7.1 | 5" x 6" x 3/8" x 3/8" | 15.65 |
IN127D | 127*152*12.7*12.7 | 9.2 | 5" x 6" x 1/2" x 1/2" | 20.28 |
IB152A | 152*305*9.5*9.5 | 10.7 | 6" x 12" x 3/8" x 3/8" | 23.68 |
IB152B | 152*305*12.7*12.7 | 14.3 | 6" x 12" x 1/2" x 1/2" | 31.53 |
Application Markets
Construction
Bridges and Highways
Chemical
Food and Beverage
Manufacturing
Metals and Mining
Microelectronics
Oil and Gas
Pharmaceutical
Power
Pulp and Paper
Recreation and Entertainment
Telecommunications
Transportation
Water and Wastewater Treatment
Features:
Corrosion-resistant
Low maintenance
Flame-retardant
Low installation cost
Heavy-metal resistant
Long service life
Electrically and thermally non-conductive
High strength-to-weight ratio
Raw material introduction — resin types
Code | Resin type | Flame-retardant performance | Recommended applications |
|---|---|---|---|
VEFR-25 | Vinyl ester type | Oxygen index 28 and above | Acid, alkali and other harsh corrosive environments |
IFR-25 | Isophthalic type | Oxygen index 28 and above | VEFR type: economical, excellent performance, resistant to moderate acids, alkalis and solvents |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | General acid and alkali environments |
Applications:
Greenlogy TEC pultruded FRP profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.
Greenlogy TEC profiles
Mechanical properties | ASTM | Unit | Value | Unit | Value |
|---|---|---|---|---|---|
Tensile stress, longitudinal (LW) | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile stress, transverse (CW) | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile modulus, longitudinal (LW) | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile modulus, transverse (CW) | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive stress, longitudinal (LW) | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive stress, transverse (CW) | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive modulus, longitudinal (LW) | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive modulus, transverse (CW) | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural stress, longitudinal (LW) | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural stress, transverse (CW) | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural modulus, longitudinal (LW) | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural modulus, transverse (CW) | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of elasticity | Full section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short-beam shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod impact strength, longitudinal | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod impact strength, transverse | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excluding round rods and square rods
Physical properties | ASTM | Unit | Value |
|---|---|---|---|
Barcol hardness | D-495 | --- | 45 |
24-hour water absorption | D-570 | % max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of thermal expansion, longitudinal | D-696 | 10^-6in./in./℃ | 8 |
Flame-retardant performance | ASTM | Unit | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame spread | Max. 25 |
Flame resistance* | D-635 | --- | Non-combustible |
Electrical properties | ASTM | Unit | Value |
|---|---|---|---|
Arc resistance, longitudinal | D-495 | 秒(s) | 120 |
Dielectric strength, LW | D-149 | kv./in. | 35 |
Dielectric strength, PF | D-149 | Volts/mil | 200 |
Dielectric constant, PF | D-150 | @60hz | 5 |
LW = longitudinal, CW = crosswise, PF = perpendicular to laminate surface
*Only applicable to ISOFR and VEFR
Application Scenarios
This product is suitable for applications requiring strength, corrosion resistance and electrical insulation, such as chemical platforms, marine engineering, power facilities, wastewater treatment and general structural support. Contact us to learn more about application cases and suitable solutions.
Selection Guide
Selection should take into account factors such as load conditions, span, corrosive environment and connection method. We can recommend suitable specifications and resin systems based on your specific operating conditions; please provide detailed parameters so that we can assist with selection.
Product Advantages
This I-beam uses an orthophthalic resin system and offers good mechanical properties, corrosion resistance and electrical insulation, along with light weight and easy installation. It is formed by the pultrusion process, with high fiber content and stable, reliable performance.
Inquiry Guidance
For detailed specifications, technical data or customized solutions, please contact us. We can provide professional support and quotations based on project requirements.
Service Environment
- This FRP I-beam is molded from glass-fiber reinforced material with resin as the binder, and is suitable for indoor and outdoor structural applications where moisture and humidity are present.
- The composite structure resists corrosion from typical industrial atmospheres and various chemical media, making it suitable for factories, walkways and platforms where steel requires frequent maintenance.
- As a non-conductive material, it can be used in locations where electrical insulation needs to be considered.
- For specific temperature limits, chemical resistance data or exposure conditions, please share your project requirements with us.