    FRP profiles are a new type of composite material made with glass fiber reinforcement as the base material, resin as the binder, and glass fiber cloth as the covering reinforcement layer; after thorough impregnation, the material is heated, formed and cured in a metal mold, and then pulled by a pultrusion (haul-off) machine. With good physical properties, it is widely used in high-strength, long-span applications.  

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Hook plate

A*B*T


A*B*T



9*70*3.2 (beveled edge)0.48

1" x 1" x 1/8" (beveled edge)

1.06

25*60*30.5

1" x 19/8" x 1/8"

1.1

25*50*3(75°)0.45

1" x 2" x 1/8" (75°)

0.99

30*70*4(90°)0.75

19/16" x 11/4" x 3/16" (90°)

1.65

30*70*3.2(90°)0.7

19/16" x 11/4" x 1/8" (90°)

1.54

30*90*3(87°)0.72

19/16" x 7/2" x 1/8" (87°)

1.59

38*230*3.2(87°)1.65

3/2" x 9" x 1/8" (87°)

3.64

40*254*6.4(87°)3.55

25/16" x 10" x 1/4" (87°)

7.83

50*140*3.2(87°)1.19

2" x 11/2" x 1/8" (87°)

2.62

55*152*3.6(87°)1.55

9/4" x 6" x 1/8" (87°)

3.42

55*230*3.6(87°)2.14

9/4" x 9" x 1/8" (87°)

4.72

55*205*3.2(87°)1.62

9/4" x 8" x 1/8" (87°)

3.57

55*55*3.2(87°)0.8

9/4" x 9/4" x 1/8" (87°)

1.76

55*70*3.2(87°)0.9

9/4" x 11/4" x 1/8" (87°)

1.98

30*76*30.6

19/16" x 3" x 1/8"

1.32

30*76*40.8

19/16" x 3" x 3/16"

1.76

25*50*3.2(90°)0.45

1" x 2" x 1/8" (90°)

0.99

25*50*4(90°)0.51

1" x 2" x 3/16" (90°)

1.12

25*100*3.2(87°)0.75

1" x 4" x 1/8" (87°)

1.65
Rounded corner30*75*3.50.69

19/16" x 3" x 1/8"

1.52
Rounded corner30*100*3.20.8

19/16" x 4" x 1/8"

1.76
Right-angled corner30*100*3.20.85

19/16" x 4" x 1/8"

1.87

30*152*3.21.2

19/16" x 6" x 1/8"

2.65
Rounded corner30*230*3.21.6

19/16" x 9" x 1/8"

3.53
Right-angled corner30*230*3.21.7

19/16" x 9" x 1/8"

3.75

55*300*4(90°)2.8

9/4" x 12" x 3/16" (90°)

6.17

55*345*4(87°)3.25

9/4" x 27/2" x 3/16" (87°)

7.17

30*381*3.2(87°)2.7

19/16" x 15" x 1/8" (87°)

5.95

55*400*3.22.8

9/4" x 63/4" x 1/8"

6.17

Markets 

  • Construction

  • Bridges and highways

  • Chemicals

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Entertainment

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Safe protection against heavy metals

  • Long service life

  • Non-conductive and thermally insulating

  • High strength-to-weight ratio

Raw material introduction — resin types

Grade

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Harsh corrosive environments such as acids and alkalis

IFR-25

Isophthalic type

Oxygen index 28 and above

Vinyl ester type, economy grade, excellent resistance to medium-concentration acids, alkalis and solvents

OFR-25

Orthophthalic

Oxygen index 28 and above

General acid and alkali environments

Applications: 

  Greenlogy TEC pultruded FRP profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight, along with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally used. Today, these profiles are commonly used in highly corrosive environments that previously required stainless steel and other expensive components.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

   Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max. 25

Non-combustibility*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Applications

FRP hook plates are commonly used for structural support and connections in corrosive environments such as chemical processing, wastewater treatment and marine engineering, and are also suitable for applications requiring insulation and non-magnetic properties. Installation is flexible, and the plates can be cut, drilled and otherwise machined to suit actual working conditions.

Selection guidance

When selecting, consider factors such as load requirements, span, corrosive environment and connection method. We recommend determining dimensions and specifications based on specific project requirements; please contact us for detailed specifications and selection advice.

Product advantages

FRP hook plates are lightweight, high-strength, corrosion-resistant, insulating and non-magnetic, and easy to install; compared with conventional metal materials, they can significantly reduce maintenance costs.

Inquiry

For detailed specifications, pricing and other commercial terms, please contact us for a tailored quotation and technical support.

Service environment

  • This FRP hook plate is a pultruded glass fiber reinforced profile, using resin as the binder and glass fiber cloth as the reinforcement layer, so it is suitable for both indoor and outdoor installation, whereas steel alternatives require frequent repainting outdoors.
  • The closed, resin-rich surface makes the hook plate a practical choice for damp or wet plant areas and environments with mildly corrosive media, where the profile serves as a connecting and supporting member rather than a decorative trim.
  • Because it is produced as a structural profile for high-strength, long-span applications, the hook plate is typically specified for chemical, water treatment, marine and general industrial environments, as well as walkway, platform and handrail assemblies.
  • The service temperature range, chemical resistance rating for specific media and allowable UV exposure depend on the resin system and actual installation; please contact us for a parameter list suitable for your project.