Product Category

Structural Profiles - Hook Plate (Isophthalic)


Contact us for a quotation

Product details

Greenlogy TEC

    FRP pultruded profiles are a new type of composite material made from glass fiber reinforcement as the raw material, resin as the binder, and glass fiber cloth as the covering reinforcement layer; after full impregnation, the material is heated, formed, and cured in a metal mold and then drawn by a pulling machine. With good physical properties, they are widely used in high-strength and long-span applications.  

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Hook plate

A*B*T


A*B*T



9*70*3.2 (beveled edge)0.48

1" x 1" x 1/8" (beveled edge)

1.06

25*60*30.5

1" x 19/8" x 1/8"

1.1

25*50*3(75°)0.45

1" x 2" x 1/8" (75°)

0.99

30*70*4(90°)0.75

19/16" x 11/4" x 3/16" (90°)

1.65

30*70*3.2(90°)0.7

19/16" x 11/4" x 1/8" (90°)

1.54

30*90*3(87°)0.72

19/16" x 7/2" x 1/8" (87°)

1.59

38*230*3.2(87°)1.65

3/2" x 9" x 1/8" (87°)

3.64

40*254*6.4(87°)3.55

25/16" x 10" x 1/4" (87°)

7.83

50*140*3.2(87°)1.19

2" x 11/2" x 1/8" (87°)

2.62

55*152*3.6(87°)1.55

9/4" x 6" x 1/8" (87°)

3.42

55*230*3.6(87°)2.14

9/4" x 9" x 1/8" (87°)

4.72

55*205*3.2(87°)1.62

9/4" x 8" x 1/8" (87°)

3.57

55*55*3.2(87°)0.8

9/4" x 9/4" x 1/8" (87°)

1.76

55*70*3.2(87°)0.9

9/4" x 11/4" x 1/8" (87°)

1.98

30*76*30.6

19/16" x 3" x 1/8"

1.32

30*76*40.8

19/16" x 3" x 3/16"

1.76

25*50*3.2(90°)0.45

1" x 2" x 1/8" (90°)

0.99

25*50*4(90°)0.51

1" x 2" x 3/16" (90°)

1.12

25*100*3.2(87°)0.75

1" x 4" x 1/8" (87°)

1.65
Rounded corner30*75*3.50.69

19/16" x 3" x 1/8"

1.52
Rounded corner30*100*3.20.8

19/16" x 4" x 1/8"

1.76
Right angle30*100*3.20.85

19/16" x 4" x 1/8"

1.87

30*152*3.21.2

19/16" x 6" x 1/8"

2.65
Rounded corner30*230*3.21.6

19/16" x 9" x 1/8"

3.53
Right angle30*230*3.21.7

19/16" x 9" x 1/8"

3.75

55*300*4(90°)2.8

9/4" x 12" x 3/16" (90°)

6.17

55*345*4(87°)3.25

9/4" x 27/2" x 3/16" (87°)

7.17

30*381*3.2(87°)2.7

19/16" x 15" x 1/8" (87°)

5.95

55*400*3.22.8

9/4" x 63/4" x 1/8"

6.17

Markets 

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Entertainment and leisure

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistance

  • Low maintenance

  • Flame retardant

  • Low installation cost

  • Heavy-metal safety

  • Long service life

  • Electrical and thermal insulation

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Harsh acid, alkali and other corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR type, economical, with good resistance to moderate acids, alkalis and solvents

OFR-25

Orthophthalic

Oxygen index 28 and above

General acid and alkali environments

Applications: 

  Greenlogy TEC pultruded FRP profiles (manufactured by Greenlogy TEC) are widely used in many fields, combining corrosion resistance, high strength, dimensional stability and light weight with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.   

Greenlogy TEC Profiles

Mechanical Properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched cantilever beam impact, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched cantilever beam impact, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

   Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max 25

Flammability performance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies only to ISOFR and VEFR


Applications

Hook plates (isophthalic) are commonly used for edge fixing on platforms in chemical, electroplating and wastewater treatment applications, connecting to grating, handrails or profiles to provide reliable support and fastening. In applications requiring high strength and corrosion resistance, such as marine engineering and oil platforms, they also offer performance advantages. Actual suitability should be assessed against specific operating conditions; contact us for application guidance.

Selection guide

When selecting, determine the hook plate dimensions (A*B*T), angle (e.g. 75° or beveled edge) and installation method to ensure compatibility with the existing structure. Isophthalic resin gives the product better corrosion resistance than orthophthalic resin, making it suitable for more demanding chemical environments. For detailed specifications and selection support, please contact us for professional advice.

Product advantages

Made with isophthalic resin, hook plates offer excellent corrosion resistance and mechanical strength, are lightweight, easy to install, and are insulating and non-magnetic. Glass fiber reinforcement ensures long-term durability, suitable for high-load and outdoor environments. We can provide customized solutions to meet your requirements; please contact us.

Inquiry

Contact us for detailed specifications, technical parameters and quotations. We provide professional selection support and customization services to meet your project requirements. Please contact us via our website or email, and we will reply as soon as possible.

Operating environment

  • Suitable for a wide range of indoor and outdoor environments; the glass fiber reinforced isophthalic resin system keeps hook plate performance stable in humid, salt-fog and general chemical corrosive atmospheres.
  • Can be used long-term from ambient to moderate temperatures for platforms, walkways and structural support applications with heat resistance requirements; ambient temperature fluctuations have little effect on the dimensional stability of the profiles.
  • Good resistance to acids, alkalis, salts and industrial atmospheres, suitable for hook plate connections and fixing in corrosive environments such as chemical plants, wastewater treatment and marine platforms.
  • Under outdoor conditions with UV exposure, use with surface protection measures is recommended to extend the service life of the hook plates and their connecting structures.