Product Category

Structural Profiles - H-Beam (Isophthalic)


Contact us for a quotation

Product details

Genius FRP  

  FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

H beam

A*B*T1*T2


A*B*T1*T2


HB76

76*76*6.4*6.4

2.67

3" x 3" x 1/4" x 1/4"

5.73

HB102A

102*102*6.4*6.4

3.59

4" x 4" x 1/4" x 1/4"

7.91

HB102B

102*102*8*8

4.5

4" x 4" x 5/16" x 5/16"

9.92

HB152A

152*152*6.4*6.4

5.43

6" x 6" x 1/4" x 1/4"

11.97

HB152B

152*152*9.5*9.5

8.1

6" x 6" x 3/8" x 3/8"

17.86

HB203A

203*203*9.5*9.5

10.8

8" x 8" x 3/8" x 3/8"

23.81

HB203B

203*203*12.7*12.7

14.4

8" x 8" x 1/2" x 1/2"

31.66

HB203C

203*203*6.4*6.4

7.5

8" x 8" x 1/4" x 1/4"

16.53

HB254A

254*254*9.5*9.5

13.6

10" x 10" x 3/8" x 3/8"

29.98

HB254B

254*254*12.7*12.7

18

10" x 10" x 1/2" x 1/2"

39.77

HB305

305*305*12.7*12.7

21.5

12" x 12" x 1/2" x 1/2"

47.4

Markets  

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

  Application:  

    Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.    

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

 Excludes Round Rod and Square Bar 

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

Structural Profile - H-Beam (Isophthalic) is suitable for applications with high requirements for corrosion resistance and strength, such as chemical platforms, wastewater treatment facilities, marine engineering, bridge walkways and long-span support structures. Its lightweight and high-strength characteristics can reduce the load on support structures and facilitate installation and maintenance.

Selection Guide

During selection, it is necessary to clarify the span, load conditions and service environment, and choose the appropriate cross-sectional dimensions based on the existing specification table. If custom cross-sections or special lengths are required, please contact us for detailed specifications and quotations.

Product Advantages

The isophthalic resin system gives the product excellent corrosion resistance and water resistance, while glass fiber reinforcement ensures high strength and stiffness. The product also features light weight, electrical insulation, non-magnetic properties and long service life, making it suitable as a replacement for traditional metal profiles.

Inquiry Guide

For detailed specifications, technical parameters or bulk purchase terms of Structural Profile - H-Beam (Isophthalic), please contact us for detailed specifications and quotations. We will provide professional advice based on your needs.

Operating Environment

  • This pultruded FRP H-beam is built on an isophthalic resin system, which makes the profile suitable for continuous service in outdoor and humid industrial settings where mild acids, alkalis and salt-laden air are present.
  • The glass fiber reinforcement and isophthalic resin matrix allow the H-beam to be used in chemical plants, wastewater areas and coastal installations where steel would require frequent recoating or replacement.
  • Because the profile is non-conductive and corrosion-resistant, it is commonly selected for indoor and outdoor structural frames, platforms and support beams exposed to weather, moisture and process spillage.
  • For applications involving concentrated chemicals, elevated temperatures or sustained load at high temperature, contact us with the specific medium and service condition so the correct resin grade and profile size can be confirmed.