Product Category

Structural Profiles - Flat Panel (Vinyl Ester)


Contact us for a quotation

Product details

Greenlogy TEC

    FRP pultruded profiles are made from glass fiber reinforcement, with resin as the binder and glass fiber cloth as the wrapping reinforcement layer; after thorough impregnation, they are heated, formed and cured in a metal mold and then pulled out by a pulling machine. As a new type of composite material with good physical properties, they are widely used in high-strength and long-span applications.  

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Flat

Thickness × Width


Thickness × Width


FP32A

3.2*1000

6.18

1/8" x 39"

13.6

FP32B

3.2*1220

7.42

1/8" x 48"

16.4

FP40A

4*800

6.2

3/16" x 32"

13.7

FP40B

4*1200

9.19

3/16" x 48"

20.3

FP48

4.8*1000

9.3

3/16" x 39"

20.5

FP50A

5*440

4.25

3/16" x 17"

9.37

FP50B

5*1220

11.8

3/16" x 48"

26

FP64

6.4*1220

14.84

1/4" x 48"

32.7

FP95

9.5*1220

22.02

3/8" x 48"

48.6

FP127

12.7*1220

29.44

1/2" x 48"

64.9

FP160

16*1220

37.2

5/8" x 48"

82

FP190

19*1220

44.1

3/4" x 48"

97.2

FP254

25.4*1220

59

1" x 48"

130

Markets 

  • Construction

  • Bridges and Highways

  • Chemical

  • Food and Beverage

  • Manufacturing

  • Metals and Mining

  • Microelectronics

  • Oil and Gas

  • Pharmaceutical

  • Power

  • Pulp and Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water and Wastewater Treatment

Features:

  • Corrosion-resistant

  • Low maintenance

  • Flame-retardant

  • Low installation cost

  • Heavy-metal-free and safe

  • Long service life

  • Non-conductive and non-thermal-conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame-retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

An economical VEFR-type product with good performance and moderate resistance to acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications:  

   Greenlogy TEC pultruded FRP profiles are used in a wide range of applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal insulation and electrical insulation properties. Where steel, aluminum or timber members have traditionally been specified, durable Greenlogy TEC profiles provide years of low-maintenance service. Today these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.   

Greenlogy TEC Profiles

Mechanical Properties

ASTM

Unit

Value

Unit

Value

Tensile Stress, Lengthwise

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, Crosswise

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, Lengthwise

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, Crosswise

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, Lengthwise

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, Crosswise

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, Lengthwise

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, Crosswise

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, Lengthwise

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, Crosswise

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, Lengthwise

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, Crosswise

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-Beam Shear Strength

D-2344

psi

4500

kgf/m²

3163813

Punch Shear Strength

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact Strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact Strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flammability performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

25 max

Combustibility*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = longitudinal, CW = transverse, PF = perpendicular to the laminate surface

*Applicable to ISOFR and VEFR only


Applications

This structural profile – flat sheet is suitable for platforms, walkways, handrails, support beams and various load-bearing structural components where strength, span and corrosion resistance are required. It can also serve as a structural alternative in corrosive environments such as chemical processing, marine and wastewater treatment. For load and span matching in specific applications, please contact us to discuss your actual working conditions.

Selection guide

When selecting, first confirm the thickness and width specifications, then evaluate the required cross-section dimensions based on the load, span and corrosion conditions of the service environment. The specifications listed in the table cover common flat sheet sizes. If the existing specifications do not fully match your needs, please contact us for detailed specifications and selection advice.

Product advantages

Made from glass fiber reinforcement with a resin matrix through a pultrusion process, it offers good physical properties and corrosion resistance, making it suitable for high-strength, long-span applications and for situations where conventional materials are prone to corrosion. Compared with metal materials, it is lighter in weight, which facilitates transport and installation. For specific performance parameters, please contact us for detailed information.

Inquiry

For detailed specifications, pricing, supply capability and other commercial terms of this structural profile – flat sheet, please contact us for detailed specifications and a quotation. Our team will provide support according to your application requirements.