Product Category

Product details

Greenlogy TEC

  FRP pultruded profiles are made from fiberglass reinforcement as the raw material, resin as the binder, and fiberglass cloth as the covering reinforcement layer; after thorough impregnation, they are heated, formed and cured in a metal mold and pulled by a pulling machine to produce a new type of composite material with good physical properties, widely used in high-strength and long-span applications.  

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Flat sheet

Thickness × Width


Thickness × Width


FP32A3.2*10006.180.59*39.3713.6
FP32B3.2*12207.420.59*48.0316.4
FP40A4*8006.20.16*31.513.7
FP40B4*12009.190.16*47.2420.3
FP484.8*10009.30.19*39.3720.5
FP50A5*4404.250.2*17.329.37
FP50B5*122011.80.2*48.0326
FP646.4*122014.840.25*48.0332.7
FP959.5*122022.020.37*48.0348.6
FP12712.7*122029.440.5*48.0364.9
FP16016*122037.20.63*48.0382
FP19019*122044.10.75*48.0397.2
FP25425.4*1220591*48.03130

Market  

  • Construction

  • Bridge and highway

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistant

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Suitable for heavy metal environments

  • Long service life

  • Electrically and thermally non-conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Standard colors

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Grass green, yellow, gray, orange

Harsh corrosive environments such as acids and alkalis

IFR-25

Isophthalic resin

Oxygen index 28 and above

Grass green, yellow, gray

VEFR type, economical, with excellent resistance to moderate acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

Grass green, yellow, gray

General acid and alkali environments

Application scenarios:

  Greenlogy TEC (Nantong Greenlogy Electronic Technology Co., Ltd.) pultruded FRP structural profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight, with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles offer years of low-maintenance service in areas where steel, aluminium or wood components are traditionally used. Today, these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.  

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal (LW)

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse (CW)

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal (LW)

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse (CW)

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal (LW)

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse (CW)

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal (LW)

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse (CW)

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal (LW)

D-790

psi

30000

kgf/m²

21092086

Flexural stress, transverse (CW)

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear test

D-732

psi

10000

kgf/m²

7030695

Notched cantilever beam impact, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched cantilever beam impact, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flammability performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

25 max

Combustibility*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

V/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Applications

Structural profiles – flat sheets are commonly used in load-bearing structures and support locations requiring high strength and larger spans, such as platform walkways, handrail frames, equipment supports and various corrosion-resistant structural components. Their glass fiber reinforcement and resin composite system make them suitable for humid conditions and corrosive media where metals are not well suited. For specific application recommendations, please contact us.

Selection guide

When selecting, start with thickness, width and unit weight, and consider span, load type and installation conditions. The specifications listed in the table can serve as an initial reference; for actual projects, we recommend providing the service environment and load requirements so we can help confirm the appropriate flat sheet specification. Please contact us for detailed specifications and a quotation.

Product advantages

This flat sheet uses glass fiber cloth as the reinforcement layer and is formed through resin impregnation, in-mold heating and curing, and pultrusion, giving it good physical properties and structural integrity. Compared with traditional metal materials, its corrosion resistance and lightweight characteristics help reduce long-term maintenance burden. Please contact us to learn about the material system and available configurations.

Inquiry

To learn about available specifications, dimensional tolerances and delivery methods for structural profiles – flat sheets, please contact us for detailed specifications and a quotation. Please provide the required thickness, width, quantity and service environment, and we will recommend a suitable solution accordingly.

Service environment

  • FRP flat structural profiles are suitable for indoor and outdoor installation, including industrial plants, chemical facilities, and coastal or marine atmospheric environments where steel would corrode.
  • Glass fiber reinforced composites with a resin matrix resist a variety of corrosive media, such as moisture, salt spray, and various acids and alkalis; for specific chemical contact, please contact us to confirm resin selection.
  • This flat profile maintains its dimensional stability under typical ambient temperature changes, without the thermal expansion or rust problems of metal profiles.
  • For continuous use in unusually high humidity, intense UV exposure or high-concentration chemical environments, please provide your project conditions so we can recommend a suitable resin system.