Structural Profiles - Curved Flat Bar (Vinyl Ester)
Product details
Greenlogy TEC
Pultruded FRP profiles are a new type of composite material made from glass fiber reinforcement, with resin as the binder and glass fiber cloth as the covering reinforcement layer. After thorough impregnation, the material is heated, formed and cured in a metal mold and then pulled by a pulling machine. With good physical properties, it is widely used in high-strength and long-span applications.
Type | Size (mm) | Weight (kg/m) | Size (in) | Weight (lbs/in) |
|---|---|---|---|---|
Fillet radius | Width × thickness | Width × thickness | ||
| FS50A | 50*3.2 | 0.29 | 2" x 1/8" | 0.64 |
| FS60A | 60*3.2 | 0.36 | 19/8" x 1/8" | 0.79 |
| FS70 | 70*4 | 0.54 | 19" x 3/16" | 1.19 |
| FS90A | 90*3.2 | 0.54 | 7/2" x 1/8" | 1.19 |
| FS100 | 100*3.2 | 0.6 | 4" x 1/8" | 1.32 |
| FS120 | 120*3 | 0.7 | 19/4" x 1/8" | 1.54 |
Markets
Construction
Bridges and highways
Chemical
Food and beverage
Manufacturing
Metals and mining
Microelectronics
Oil and gas
Pharmaceutical
Power
Pulp and paper
Recreation
Telecommunications
Transportation
Water and wastewater treatment
Features:
Corrosion resistance
Low maintenance cost
Flame retardant
Low installation cost
Heavy metal resistance
Long service life
Non-conductive and non-heat-conductive
High strength-to-weight ratio
Raw material introduction — resin types
Code | Resin type | Flame retardant performance | Recommended applications |
|---|---|---|---|
VEFR-25 | Vinyl ester type | Oxygen index 28 and above | Severe acid, alkali and other corrosive environments |
IFR-25 | Isophthalic type | Oxygen index 28 and above | VEFR type, economical grade with good performance, resistant to moderate acids, alkalis and solvents |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | General acid and alkali environments |
Applications:
Greenlogy TEC pultruded FRP profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight, with thermal insulation and non-conductive properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in applications where steel, aluminum or wood components have traditionally been used. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.
Greenlogy TEC Profiles
Mechanical Properties | ASTM | Unit | Value | Unit | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact, Longitudinal (LW) | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact, Transverse (CW) | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excluding round rods and square rods
Physical properties | ASTM | Unit | Value |
|---|---|---|---|
Barcol hardness | D-495 | --- | 45 |
24-hour water absorption | D-570 | Maximum value % | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of thermal expansion, longitudinal (LW) | D-696 | 10^-6in./in./℃ | 8 |
Flame retardant performance | ASTM | Unit | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame spread | Maximum 25 |
Combustibility* | D-635 | --- | Non-combustible |
Electrical properties | ASTM | Unit | Value |
|---|---|---|---|
Arc resistance, LW | D-495 | 秒(s) | 120 |
Dielectric strength, LW | D-149 | kv./in. | 35 |
Dielectric strength, PF | D-149 | Volts/mil | 200 |
Dielectric constant, PF | D-150 | @60hz | 5 |
LW = longitudinal, CW = transverse, PF = perpendicular to the laminate surface
*Applicable to ISOFR and VEFR only
Applications
Structural Profiles – Curved Flat Bar (Vinylester) is suitable for platforms, walkways, handrails and curved structural supports where corrosion resistance and light weight are required, and is often used together with grating and pultruded profiles. To confirm suitability for your specific service conditions, contact us for detailed specifications and selection advice.
Selection Guidance
When selecting, consider the curve radius, section width and thickness, load-bearing span and installation method together, and ensure compatibility with adjacent components. As multiple specification combinations are involved, contact us for detailed specifications and a quotation, and our technical staff will help confirm a suitable model.
Product Advantages
This profile is pultruded from glass fiber reinforcement and resin, offering light weight, high strength, corrosion resistance, electrical insulation and dimensional stability, making it suitable for high-strength, long-span applications. The vinylester system helps improve resistance to chemical media; actual performance varies with the service environment.
Inquiry
For information on available specification ranges, surface treatment options and delivery arrangements, contact us for detailed specifications and a quotation. Please provide the required section dimensions, curvature requirements and service environment, and we will respond with a corresponding solution.
Service Environment
- Vinylester glass fiber structural profile formulations are suitable for long-term outdoor exposure and resist UV degradation and weathering in industrial and marine atmospheric environments.
- These pultruded profiles can withstand humid, immersed and salt-bearing environments without the corrosion that affects steel, making them suitable for coastal, offshore and chemical plant environments.
- When vinylester resin is selected, they can withstand splashes and vapors of acids, alkalis and solvents; however, direct contact with concentrated or high-temperature chemical fluids should be confirmed against the project's media list.
- Typical installations include walkways, platforms, handrails and cable trays in wastewater treatment, chemical processing and offshore structures, where the profiles remain stable under outdoor temperature fluctuations and condensation.