Structural Profiles - Angle (Orthophthalic)


Contact us for a quotation

Product details

Greenlogy TEC

  FRP pultruded profiles are made from glass fiber reinforcement, with resin as the binder and glass fiber cloth as the wrapping reinforcement layer; after thorough impregnation, they are heated, formed and cured in a metal mold and pulled out by a pulling machine. This new composite material has good physical properties and is widely used in high-strength and long-span applications.  

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Angle

A*B*T1*T2
A*B*T1*T2
EL25A25*25*3.2*3.20.331" x 1" x 1/8" x 1/8"0.73
EL25B25*25*6.4*6.40.561" x 1" x 1/4" x 1/4"1.23
EL30A30*30*4(75°)0.46

5/4" x 5/4" x 3/16" (75°)

1.01
EL30B30*30*5*50.57

5/4" x 5/4" x 3/16" x 3/16"

1.26
EL3232*32*4*40.42

5/4" x 5/4" x 3/16" x 3/16"

0.93
EL38A38*38*5*50.68

3/2" x 3/2" x 3/16" x 3/16"

1.5
EL38B38*38*6.4*6.40.85

3/2" x 3/2" x 1/4" x 1/4"

1.87
EL4545*45*4.8*4.80.75

7/4" x 7/4" x 3/16" x 3/16"

1.65
EL50A50*50*3.2*3.20.62

2" x 2" x 1/8" x 1/8"

1.37
EL50B50*50*6.4*6.41.14

2" x 2" x 1/4" x 1/4"

2.51
EL6060*60*9*91.9

19/8" x 19/8" x 3/8" x 3/8"

4.19
EL76A76*76*4.8*4.81.38

3" x 3" x 3/16" x 3/16"

3.04
EL76B76*76*6.4*6.41.77

3" x 3" x 1/4" x 1/4"

3.9
EL76C76*76*9.5*9.52.57

3" x 3" x 3/8" x 3/8"

5.67
EL76D76*76*12.7*12.73.4

3" x 3" x 1/2" x 1/2"

7.5
EL101A101*101*6.4*6.42.5

4" x 4" x 1/4" x 1/4"

5.51
EL101B101*101*8*82.95

4" x 4" x 5/16" x 5/16"

6.5
EL101C101*101*9.5*9.53.48

4" x 4" x 3/8" x 3/8"

7.67
EL101D101*101*12.7*12.74.57

4" x 4" x 1/2" x 1/2"

10.1
EL152A152*152*6.4*6.43.62

6" x 6" x 1/4" x 1/4"

7.98
EL152B152*152*9.5*9.55.42

6" x 6" x 3/8" x 3/8"

12
EL152C152*152*12.7*12.77.01

6" x 6" x 1/2" x 1/2"

15.5
L4040*22*4.0*4.00.45

25/16" x 7/8" x 3/16" x 3/16"

0.99
L7676*15*6*60.98

3" x 9/16" x 1/4" x 1/4"

2.16
L100100*50*6.4*6.41.8

4" x 2" x 1/4" x 1/4"

3.97
L145145*76*10*103.85

23/4" x 3" x 3/8" x 3/8"

8.49
L170170*76*9.5*9.54.4

27/4" x 3" x 3/8" x 3/8"

9.7
L180180*80*8.0*8.03.89

7" x 25/8" x 5/16" x 5/16"

8.58
L254254*40*6.4*6.43.61

10" x 25/16" x 1/4" x 1/4"

7.96
L70 (special)70*70*24*6.03.75

11/4" x 11/4" x 15/16" x 1/4"

8.27

Markets 

  • Construction

  • Bridges & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gas

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater Treatment

Features:

  • Corrosion resistant

  • Low maintenance

  • Flame retardant

  • Low installation cost

  • Safe in heavy-metal environments

  • Long service life

  • Non-conductive and thermally insulating

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardancy

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR grade, economical, good performance, resistant to moderate acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications:

  Greenlogy TEC pultruded FRP structural profiles are used in a wide range of applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal insulation and non-conductive properties. Durable Greenlogy TEC profiles provide years of low-maintenance performance in areas where steel, aluminum or wood components are traditionally specified. Today these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.  

Greenlogy TEC profiles

Mechanical Properties

ASTM

Unit

Value

Unit

Value

Tensile Stress, Longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, Transverse

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, Longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, Transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, Longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, Transverse

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, Longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, Transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, Longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, Transverse

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, Longitudinal

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, Transverse

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardancy

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

25 max

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

V/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate face

*Only applicable to ISOFR and VEFR


Application scenarios

FRP angle is commonly used in chemical, wastewater treatment, marine engineering, power and general corrosive environments for platform supports, guardrail frames, cable tray supports and structural reinforcement. Its orthophthalic resin system suits most routine industrial corrosive conditions; for special media such as strong acids, strong alkalis or high temperatures, please contact us with your operating environment so we can recommend a more suitable resin system.

Selection guide

When selecting, first confirm equal or unequal leg, leg width and thickness, then determine the cross-section specification based on span, load direction and connection method; A*B*T1*T2 in the table represent the two leg lengths and their corresponding thicknesses. As FRP is an anisotropic material, we recommend having us verify the load and deflection requirements before finalizing the model; please contact us with your operating parameters for selection advice.

Product advantages

Pultruded FRP angle uses glass fiber as reinforcement and resin as matrix, formed by continuous pultrusion with heat curing. It features light weight and high strength, corrosion resistance, no rusting, non-magnetic and insulating properties, and is easy to cut and drill on site. Compared with traditional steel, it can reduce maintenance and replacement frequency in corrosive environments, making it suitable for applications with both weight and durability requirements.

Inquiry guidance

For specific specifications, dimensional tolerances, surface treatment, packaging and delivery lead times of structural profiles - angle (orthophthalic), please contact us for detailed specifications and quotations. Please also inform us of the required model, quantity, operating environment and delivery destination, and we will provide a targeted solution and commercial terms accordingly.

Operating environment

  • This FRP angle uses orthophthalic resin and glass fiber reinforcement, suitable for outdoor and indoor structural frames, especially where conventional steel angle would corrode under humid and atmospheric exposure conditions.
  • Typical installation locations include chemical plants, water treatment areas and coastal or humid industrial sites, where the profiles resist splashes, steam and mildly corrosive media without rusting like metal angles.
  • The pultruded glass fiber structure keeps the angle stable within the normal service temperature range of industrial buildings and open-air structures, from cold workshops to sun-exposed platforms.
  • For continuous immersion, strong solvents or concentrated acid environments, or for load-bearing design, please inform us of your operating conditions so we can confirm the correct resin grade and profile.