Structural Profiles - Angle (Isophthalic)
Product details
Greenlogy TEC
FRP pultruded profiles use glass fiber reinforcement as the base material, resin as the binder, and glass fiber cloth as the covering reinforcement layer. After thorough impregnation, they are heated, formed, and cured in a metal mold and pulled in a haul-off machine. This is a new type of composite material with good physical properties, widely used in high-strength, large-span working conditions.
Type | Size (mm) | Weight (kg/m) | Size (in) | Weight (lbs/in) |
|---|---|---|---|---|
Angle | A*B*T1*T2 | A*B*T1*T2 | ||
| EL25A | 25*25*3.2*3.2 | 0.33 | 1" x 1" x 1/8" x 1/8" | 0.73 |
| EL25B | 25*25*6.4*6.4 | 0.56 | 1" x 1" x 1/4" x 1/4" | 1.23 |
| EL30A | 30*30*4(75°) | 0.46 | 5/4" x 5/4" x 3/16" (75°) | 1.01 |
| EL30B | 30*30*5*5 | 0.57 | 5/4" x 5/4" x 3/16" x 3/16" | 1.26 |
| EL32 | 32*32*4*4 | 0.42 | 5/4" x 5/4" x 3/16" x 3/16" | 0.93 |
| EL38A | 38*38*5*5 | 0.68 | 3/2" x 3/2" x 3/16" x 3/16" | 1.5 |
| EL38B | 38*38*6.4*6.4 | 0.85 | 3/2" x 3/2" x 1/4" x 1/4" | 1.87 |
| EL45 | 45*45*4.8*4.8 | 0.75 | 7/4" x 7/4" x 3/16" x 3/16" | 1.65 |
| EL50A | 50*50*3.2*3.2 | 0.62 | 2" x 2" x 1/8" x 1/8" | 1.37 |
| EL50B | 50*50*6.4*6.4 | 1.14 | 2" x 2" x 1/4" x 1/4" | 2.51 |
| EL60 | 60*60*9*9 | 1.9 | 19/8" x 19/8" x 3/8" x 3/8" | 4.19 |
| EL76A | 76*76*4.8*4.8 | 1.38 | 3" x 3" x 3/16" x 3/16" | 3.04 |
| EL76B | 76*76*6.4*6.4 | 1.77 | 3" x 3" x 1/4" x 1/4" | 3.9 |
| EL76C | 76*76*9.5*9.5 | 2.57 | 3" x 3" x 3/8" x 3/8" | 5.67 |
| EL76D | 76*76*12.7*12.7 | 3.4 | 3" x 3" x 1/2" x 1/2" | 7.5 |
| EL101A | 101*101*6.4*6.4 | 2.5 | 4" x 4" x 1/4" x 1/4" | 5.51 |
| EL101B | 101*101*8*8 | 2.95 | 4" x 4" x 5/16" x 5/16" | 6.5 |
| EL101C | 101*101*9.5*9.5 | 3.48 | 4" x 4" x 3/8" x 3/8" | 7.67 |
| EL101D | 101*101*12.7*12.7 | 4.57 | 4" x 4" x 1/2" x 1/2" | 10.1 |
| EL152A | 152*152*6.4*6.4 | 3.62 | 6" x 6" x 1/4" x 1/4" | 7.98 |
| EL152B | 152*152*9.5*9.5 | 5.42 | 6" x 6" x 3/8" x 3/8" | 12 |
| EL152C | 152*152*12.7*12.7 | 7.01 | 6" x 6" x 1/2" x 1/2" | 15.5 |
| L40 | 40*22*4.0*4.0 | 0.45 | 25/16" x 7/8" x 3/16" x 3/16" | 0.99 |
| L76 | 76*15*6*6 | 0.98 | 3" x 9/16" x 1/4" x 1/4" | 2.16 |
| L100 | 100*50*6.4*6.4 | 1.8 | 4" x 2" x 1/4" x 1/4" | 3.97 |
| L145 | 145*76*10*10 | 3.85 | 23/4" x 3" x 3/8" x 3/8" | 8.49 |
| L170 | 170*76*9.5*9.5 | 4.4 | 27/4" x 3" x 3/8" x 3/8" | 9.7 |
| L180 | 180*80*8.0*8.0 | 3.89 | 7" x 25/8" x 5/16" x 5/16" | 8.58 |
| L254 | 254*40*6.4*6.4 | 3.61 | 10" x 25/16" x 1/4" x 1/4" | 7.96 |
| L70 (special) | 70*70*24*6.0 | 3.75 | 11/4" x 11/4" x 15/16" x 1/4" | 8.27 |
Markets
Construction
Bridges and highways
Chemical
Food and beverage
Manufacturing
Metals and mining
Microelectronics
Oil and gas
Pharmaceutical
Power
Pulp and paper
Recreation and leisure
Telecommunications
Transportation
Water and wastewater treatment
Features:
Corrosion resistant
Low maintenance
Flame retardant
Low installation cost
Heavy metal resistant
Long service life
Electrical and thermal insulation (non-conductive)
High strength-to-weight ratio
Raw material introduction — resin types
Code | Resin type | Flame retardant performance | Recommended applications |
|---|---|---|---|
VEFR-25 | Vinyl ester type | Oxygen index 28 and above | Acid, alkali and other harsh corrosive environments |
IFR-25 | Isophthalic type | Oxygen index 28 and above | A cost-effective VEFR-grade resin with good performance and moderate resistance to acids, alkalis and solvents |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | General acid and alkali environments |
Applications:
Pultruded FRP profiles from Greenlogy TEC (Nantong Greenlogy Electronic Technology Co., Ltd.) are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal insulation and non-conductivity. Durable Greenlogy TEC profiles deliver years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today, these profiles are often used in highly corrosive environments that previously required stainless steel and other costly components.
Greenlogy TEC profiles
Mechanical Properties | ASTM | Unit | Value | Unit | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 |
10^6kgf/m² | 562 |
Elastic Modulus | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short-Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact, LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact, CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excluding round rods and square rods
Physical Properties | ASTM | Unit | Value |
|---|---|---|---|
Barcol hardness | D-495 | --- | 45 |
24-hour water absorption | D-570 | Max. % | 0.45 |
Density |
D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of thermal expansion, LW | D-696 | 10^-6in./in./℃ | 8 |
Flame retardant performance | ASTM | Unit | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame spread | Max. 25 |
Flame resistance* | D-635 | --- | Non-combustible |
Electrical properties | ASTM | Unit | Value |
|---|---|---|---|
Arc resistance, LW | D-495 | 秒(s) | 120 |
Dielectric strength, LW | D-149 | kv./in. | 35 |
Dielectric strength, PF | D-149 | V/mil | 200 |
Dielectric constant, PF | D-150 | @60hz | 5 |
LW = lengthwise, CW = crosswise, PF = perpendicular to laminate face
*Only applicable to ISOFR and VEFR
Application Scenarios
Structural Profile - Angle (Isophthalic) is suitable for corrosive environments such as chemical, marine and wastewater treatment, as well as structural support applications requiring high strength and large spans. The isophthalic resin gives it excellent corrosion resistance and weather resistance, maintaining stability during long-term use outdoors and in damp conditions. Welcome to contact us to learn about the suitability of this product for your specific project.
Selection Guide
When selecting, please determine the specification and dimensions of the angle according to design loads, spans and connection methods. Different leg widths and thicknesses correspond to different load-bearing capacities, and the isophthalic resin type can meet higher corrosion resistance requirements. For precise selection advice, welcome to contact us for detailed specifications and technical support.
Product Advantages
Compared with traditional metal materials, FRP angles feature light weight, high strength, corrosion resistance, insulation and non-magnetic properties, and are easy to cut and install. The isophthalic resin system further improves the product's chemical resistance and durability, making it suitable for demanding industrial environments. Welcome to contact us for more information on product advantages.
Inquiry Guide
For detailed specifications, prices and supply information on Structural Profile - Angle (Isophthalic), welcome to contact us. We can provide customized solutions according to your project requirements. Please submit your inquiry via the website or email, and we will reply as soon as possible.
Operating Environment
- FRP angles (isophthalic resin type) are suitable for indoor and outdoor structural applications in industrial, marine and chemical processing environments.
- The isophthalic resin matrix offers enhanced resistance to water, moisture and a variety of corrosive media, making these profiles suitable for washdown areas, wastewater treatment plants and coastal facilities.
- These FRP angle profiles perform well across the wide temperature range typical of industrial use (from low sub-zero temperatures to higher process temperatures) without compromising mechanical integrity.
- The formulation contains UV stabilizers, enabling the angles to resist degradation caused by sunlight and weathering and ensuring long-term durability of exposed outdoor structural systems.