Product Category

Product details

Greenlogy TEC

  FRP pultruded grating is made from pultruded "I"-shaped and "T"-shaped profiles as bearing bars, with solid tubes or rods as connecting rods, assembled per a defined assembly process into grating with gaps in the panel surface.  

Name

Content

Type

Resin

25%

OFR-25,IFR-25,VEFR-25

Glass fiber

65%

E

Filler

8%

ATH,PR

Others

2%

---

Raw material introduction 
Resin type

Code

Resin type

Flame retardant performance

Recommended application

MP-5

Phenolic type

Oxygen index up to approximately 80

Low toxicity and high flame retardancy; suitable for applications with high fire safety requirements

VEFR-25

Vinyl ester type

Oxygen index above 28

Harsh environments with strong corrosive media such as acids and alkalis

VEFR-10

Vinyl ester type

Oxygen index above 35

Applications requiring high flame retardancy with strong acids, strong alkalis and favorable service conditions

IFR-25

Isophthalic type

Oxygen index above 28

VEFR economical grade, good performance, resistant to moderate acids, alkalis and solvents

IFGR-30

Styrene food grade

Oxygen index 26

Mainly used in meat processing and food processing plants

OFR-25

Orthophthalic type

Oxygen index above 28

General acid and alkali environments

OCR

Orthophthalic type

Oxygen index below 28

OFR-25 economical grade, no flame retardancy requirement

Coarse glass fiber selection  

Code

Coarse sand grade

Recommended application

E

E-glass fiber

For high-strength requirements and highly corrosive environments

Filler type selection 

Code

Filler type

Recommended application

ATH

Aluminum hydroxide

Flame-retardant, smoke-suppressing and corrosion-resistant applications

PR

No filler, pure resin

For highly corrosion-resistant applications

Sand surface

Smooth surface

Anti-slip grooved surface

Standard panel size:
1220mm, 915mm width; 3050mm, 6100mm length
Load-bearing flat bar: 38mm
Open area: 12%

Approx. weight (including three-core strand): 19.6kg/m²

Linear load (unit: mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Ultimate

(mm)

15030045075015003000

load

450<0.250.250.250.511.021.788791
600<0.250.250.510.761.783.567033
9000.511.021.522.795.3310.74679
12001.272.543.566.112.2---3516

Uniformly distributed load (unit: mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Ultimate

(mm)

4509501450240048509500

load

450<0.250.250.250.511.021.7819227
6000.250.510.761.022.294.3214396
9001.022.033.055.0810.2---9614
12003.056.19.14---------5758

Features:

  • Flame retardant

  • High flame retardancy

  • Low smoke and low-toxicity emissions

  • High strength-to-weight ratio

  • Corrosion resistant

  • Low maintenance

  • Anti-slip

  • Non-conductive and non-heat-conductive

  • Easy to process

  • Impact resistance 

  • UV resistance

  • Maintenance-free

Installation and accessories  


Application scenarios

Pultruded grating T-1215 uses pultruded I-profiles and T-profiles as load-bearing bars, with solid tubes or rods as connecting rods. It is suitable for platforms, walkways, trench covers, stair treads and similar applications that require both load-bearing capacity and corrosion resistance. In humid or corrosive environments such as chemical processing, water treatment, electroplating and marine engineering, it can serve as an alternative to conventional metal grating. To confirm suitability for your specific operating conditions, please contact us with details of your service environment.

Selection guidance

Selection can be considered from several aspects: resin system, load-bearing direction, span and installation method. The resin type must match the corrosiveness and flame-retardant requirements of the environment; the specification and spacing of the load-bearing bars determine the load capacity; and the type of connecting rods affects overall stiffness. Different resin and fiber ratios correspond to different corrosion resistance and flame-retardant performance. We recommend providing the service medium, temperature range and load conditions so that we can help recommend a suitable configuration.

Product advantages

The pultrusion process arranges fibers continuously along the load direction, giving the product high strength and stiffness in the load-bearing direction, along with the common advantages of FRP materials: light weight, corrosion resistance and maintenance-free performance. The grating surface can be made in an anti-slip form, and it is easy to cut and adjust on site during installation. It does not rust easily over long-term use. Compared with molded grating, pultruded grating is better suited to applications with load and span requirements.

Inquiry guidance

For detailed specifications, resin options and supply information for pultruded grating T-1215, please contact us to obtain detailed specifications and a quotation. Please provide information such as the service environment, load requirements, dimensions and quantity, and we will provide targeted recommendations and commercial terms accordingly.