Product details
Product Details
6x37 Specifications Generally used for cross lay in engineering, also available with FC (imported hemp core). 6x36 is more popular in the UK; while in continental Europe,6x37 is generally used.
Surface treatment: bright or galvanized
Standard: GB/T 20118-2006
Engineering Applications
General engineering wire rope
Crane wire rope
Sling
Breaking load
|
|
Minimum breaking load | Minimum breaking load |
Minimum breaking load | Minimum breaking load |
|---|---|---|---|---|---|
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 12 | 0.5 | 75.2 | 7669 | 83.3 | 8492 |
| 13 | 0.59 | 88.2 | 9000 | 97.7 | 9967 |
| 14 | 0.68 | 102 | 10438 | 113 | 11559 |
| 16 | 0.89 | 134 | 13634 | 148 | 15098 |
| 18 | 1.12 | 169 | 17256 | 187 | 19108 |
| 20 | 1.38 | 209 | 21303 | 231 | 23590 |
| 22 | 1.68 | 253 | 25777 | 280 | 28544 |
| 24 | 1.99 | 301 | 30677 | 333 | 33970 |
| 26 | 2.34 | 353 | 36003 | 391 | 39868 |
| 28 | 2.71 | 409 | 41755 | 453 | 46237 |
| 30 | 3.11 | 470 | 47933 | 520 | 53078 |
| 32 | 3.54 | 535 | 54537 | 592 | 60391 |
| 34 | 4 | 604 | 61567 | 668 | 68176 |
| 36 | 4.48 | 677 | 69024 | 749 | 76433 |
| 38 | 5 | 754 | 76906 | 835 | 85161 |
| 40 | 5.54 | 835 | 85214 | 925 | 94362 |
| 42 | 6.1 | 921 | 93949 | 1020 | 104034 |
| 44 | 6.7 | 1011 | 103110 | 1119 | 114178 |
| 46 | 7.32 | 1105 | 112696 | 1224 | 124794 |
| 48 | 7.97 | 1203 | 122709 | 1332 | 135881 |
General engineering wire rope
Greenlogy TEC LM specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these conventional wire ropes, we can also supply high-quality specialty wire ropes.
Most wire ropes work under demanding conditions and must be resistant to crushing, bending fatigue and wear. All our wire ropes strive for a high performance level to extend service life, thereby improving end-user productivity. We therefore ensure all materials are produced in accordance with wire rope industry standards. Each wire rope can be supplied with assembly components such as thimbles, swaged ends and wedge sockets as well as many others. In addition, we offer customization services - our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable and comply with ISO9001.
Selection Guide
When selecting, first confirm the application scenario and load requirements, then match them against the diameter, weight and minimum breaking load corresponding to different strength grades in the table. Surface treatment options include bright or galvanized, and core options include FC imported hemp core. For specific specifications and recommendations on matching working conditions, please contact us for detailed specifications and quotations.
Product Advantages
This product is manufactured in accordance with GB/T 20118-2006. The 6x37 construction offers good flexibility, making it suitable for general engineering, cranes and slings, with an optional imported FC hemp core to enhance performance. For material certificates, test reports and other documents, please contact us for detailed specifications and a quotation.
Inquiry Guidance
If you would like to learn about available diameter ranges, surface finishes, core options and commercial terms such as packaging and shipping, please provide your application conditions and required quantity. Please contact us for detailed specifications and a quotation.
Operating Environment
- LM Wire Rope GB 6x37 FC is a general engineering wire rope suited to both indoor plant installations and outdoor service, where the bright or galvanized surface treatment is selected according to the atmosphere.
- With its fiber core and 6x37 strand construction, it is used in crane, sling and general engineering duty where the rope bends over sheaves and drums and must remain flexible in service.
- For humid, marine or chemically aggressive surroundings, the galvanized option is normally specified to resist corrosion of the steel wires; the fiber core should not be relied on where sustained high temperature or direct chemical attack is present.
- As with any wire rope, service life depends on the actual working environment, so buyers should confirm the surface treatment and core type against their site conditions before ordering.