Product details
Product Details
1x19 Galvanized Steel Wire Rope Attractive appearance,with excellent breaking load capacity and low elongation characteristics, it is the most popular among small-diameter wire ropes.
Surface treatment: bright or galvanized
Standard: GB/T 20118-2006
Engineering Applications
Construction engineering applications
Small-diameter wire rope slings
Guy wires
Fencing wire rope
Slings
Garage door wire rope
Fixed guy wires
Tag hanging ropes
Cable car ropes
Breaking load
|
|
Minimum breaking load | Minimum breaking load |
Minimum breaking load | Minimum breaking load |
|---|---|---|---|---|---|
Diameter | Weight | (1770Mpa) | (1770Mpa) | (1960Mpa) | 1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 1 | 0.005 | 0.93 | 95 | 1.03 | 105 |
| 1.2 | 0.007 | 1.34 | 136 | 1.48 | 151 |
| 1.5 | 0.01 | 2.09 | 213 | 2.32 | 236 |
| 1.8 | 0.016 | 3.01 | 307 | 3.33 | 340 |
| 2 | 0.02 | 3.72 | 379 | 4.12 | 420 |
| 2.3 | 0.026 | 4.92 | 501 | 5.44 | 555 |
| 2.5 | 0.03 | 5.81 | 592 | 6.43 | 656 |
| 3 | 0.05 | 8.36 | 853 | 9.26 | 944 |
| 4 | 0.08 | 14.9 | 1516 | 16.5 | 1678 |
| 5 | 0.12 | 23.2 | 2368 | 25.7 | 2622 |
| 6 | 0.18 | 33.5 | 3410 | 37 | 3776 |
| 7 | 0.24 | 45.5 | 4642 | 50.4 | 5140 |
| 8 | 0.32 | 59.5 | 6062 | 65.9 | 6713 |
| 9 | 0.4 | 75.3 | 7673 | 83.3 | 8496 |
| 10 | 0.5 | 92.9 | 9472 | 103 | 10489 |
| 11 | 0.6 | 112 | 11462 | 125 | 12692 |
| 12 | 0.71 | 134 | 13640 | 148 | 15105 |
| 14 | 0.97 | 182 | 18566 | 202 | 20559 |
| 16 | 1.27 | 238 | 24250 | 263 | 26853 |
| 19 | 1.79 | 335 | 34196 | 371 | 37866 |
| 22 | 2.4 | 450 | 45847 | 498 | 50768 |
| 26 | 3.35 | 628 | 64034 | 696 | 70908 |
General engineering wire rope
Greenlogy TEC specializes in supplying multi-strand bright or galvanized steel wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these conventional wire ropes, we can also supply premium special wire ropes.
Most wire ropes work under demanding conditions and must possess resistance to crushing, bending fatigue, and abrasion. All our wire ropes strive to achieve a high level of performance to extend service life, thereby improving end-user productivity. We therefore ensure all materials are produced in accordance with wire rope industry standards. Each wire rope can be supplied with fittings such as thimble eyes, swaged ends, and wedge sockets, as well as many other assembly components. In addition, we offer customization services: our engineering team can manufacture wire ropes to the specifications you require. All materials are certified, traceable, and compliant with ISO9001.
Selection Guide
1x19 structural wire rope has high rigidity, high breaking load, and low elongation, making it suitable for slings, stays, and fixed guy ropes where dimensional stability is required. When selecting, please consider the required diameter, surface finish (bright or galvanized), and the breaking load requirements for the actual working conditions. Please contact us for detailed specifications and selection advice.
Product Advantages
1x19 galvanized wire rope has an attractive appearance and combines excellent breaking load capacity with low elongation, making it a popular structural form among small-diameter wire rope constructions. Its dense strand structure deforms little under high tensile loads, making it suitable for construction, rigging, and various fixed support applications.
Inquiry Guide
For specific diameters, surface finishes, or bulk supply, please contact us for detailed specifications and a quotation. Please provide information such as the required diameter, surface finish, and application, and we will recommend suitable products and reply with commercial terms accordingly.
Operating Environment
- As a galvanized or bright 1x19 steel wire rope, this product is suited to both indoor and outdoor service; the galvanized surface treatment is the usual choice where the rope is exposed to weather or moisture.
- Typical uses such as guy wires, fencing wire rope, fixed guy wires, garage door wire rope and tag hanging ropes place the rope in general outdoor and workshop atmospheres, where humidity and intermittent wetting are expected.
- Because 1x19 is a strand construction with low elongation and high breaking load for its small diameter, it is commonly selected for tensioned static duties rather than for running over sheaves, so the environment it sees should be free of repeated flexing around small drums.
- For service in aggressive corrosive media, elevated temperature or other demanding conditions, confirm the appropriate surface treatment and specification with us before ordering.